Title: Experiences in the Use of Superplasticizers in Germany

Author(s): A. Meyer

Publication: Symposium Paper

Volume: 62

Issue:

Appears on pages(s): 21-36

Keywords: admixtures; compressive strength; concrete construction; concretes; fresh concretes; plasticizers; plastics, polymers and resins; specifications; water-cement ratio; water content; water-reducing agents; workability

DOI: 10.14359/17717

Date: 1/1/1979

Abstract:
Admixtures that fulidify concrete have been used in Germany for many years to improve the workability of concrete and to reduce its water content. However, in the 1960's more effective fluidifiers were introduced in Germany and are known as superplasticizers. The real breakthrough in the application of these new types of admixtures came during the early 1970s.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer