Title: The Anchorage of Engineered Structures to Concrete and Other Foundations

Author(s): John J. White

Publication: Symposium Paper

Volume: 22

Issue:

Appears on pages(s): 171-202

Keywords: adhesives; anchorage; anchors; bascule bridges; blast reistant concstruction; bolts; bonding strength; bridge anchorages; bridges (structures); buildings; cantilever bridges; columns (structural); concretes; connections; construction; damns

DOI: 10.14359/17562

Date: 1/1/1969

Abstract:
In this paper achorages of engineered structures to concrete and other foundations are treated as arrangements for exerting restraint through resistance to stresses in shear, tension, and compression.




  