Title: Methods of Evaluation of Epoxy Compounds used for Bonding Concrete
Author(s): J.D. Kriegh and G.M. Nordby
Publication: Symposium Paper
Volume: 21
Issue:
Appears on pages(s): 107-118
Keywords:
DOI: 10.14359/17548
Date: 1/1/1968
Abstract: Test methods for evaluating epoxy compounds used for bonding concrete are discussed. . .Recommendations are made for use and development of this test procedure as a standard.