Title: Repair of Cavitation Damage in Concrete with Epoxy Resin Materials
Author(s): H.B. Erickson
Publication: Symposium Paper
Volume: 21
Issue:
Appears on pages(s): 67-78
Keywords:
DOI: 10.14359/17545
Date: 1/1/1968
Abstract: Portland-cement concreet in the floor of the outlet works at Fort Randall Dam, Pickstown, South Dakota was damaged by cavitation from high-velocity water flow. An engineering study indicated that repair could be accomplished most economically with epoxy-resin materials.