Title: Initial and Time-Dependent Shear Deflection of Reinforced Concrete T-Beams

Author(s): W.H. Dilger and G. Abele

Publication: Symposium Paper

Volume: 43

Issue:

Appears on pages(s): 487-514

Keywords: bending moments; cracking (fracturing); creep properties; deflection; deformation; flexural strength; loads (forces); reinforced concrete; shear properties; shrinkage; stirrups; T-beams; trusses; webs (supports)

DOI: 10.14359/17523

Date: 1/1/1974

Abstract:
An experimental investigation into the deformations of reinforced concrete T-beams subjected to sustained load is reported.




  