Compressive Membrane Enhancement in Two-Way Bridge Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compressive Membrane Enhancement in Two-Way Bridge Slabs

Author(s): P.Y. Tong and B deV. Batchelor

Publication: Symposium Paper

Volume: 30

Issue:

Appears on pages(s): 271-286

Keywords: bridge decks; concrete slabs; continuity (structural); flexural strength; isotropy; loads (forces); models; punching shear; reinforced concrete; research; restraints; shear properties; strength; structural design; two-way slabs; yield-line method

DOI: 10.14359/17499

Date: 1/1/1971

Abstract:
The results of a study of the ultimate strength of istropically reinforced continuous two-way bridge slabs, subjected to concentrated wheel loads, are reported. A theory is proposed for predicting the ultimate strength of such slabs, which includes the enhancement in strength due to compressive membrane action.