Title: Studies of Creep in Mass Concrete

Author(s): Milos Polivka, David Pirtz, and Robert F. Adams

Publication: Symposium Paper

Volume: 6

Issue:

Appears on pages(s): 257-286

Keywords:

DOI: 10.14359/17327

Date: 1/1/1963

Abstract:
A study of the creep characteristics of mass concrete carried out at the University of California to determine stress from strain measurements and to determine the sustained modulus of elasticity for the design of mass concrete structures.




  