Wedge-Type Expansion Anchor Performance in Tension

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Wedge-Type Expansion Anchor Performance in Tension

Author(s): Frank G. Schwarz

Publication: Symposium Paper

Volume: 103

Issue:

Appears on pages(s): 89-106

Keywords: anchors (fasteners); concretes; embedment; expansion; failure; performance; pullout tests; tension; Construction

DOI: 10.14359/1722

Date: 9/1/1987

Abstract:
The paper discusses the results of a test program comprised of 60 tensile tests of wedge-type expansion anchors installed in uncracked concrete. Typical anchor performance is analyzed during the installation, intermediate loading, and ultimate failure sta




  