Title: Mechanisms of Creep in Concrete

Author(s): lqbal Ali and Clyde E. Kesler

Publication: Symposium Paper

Volume: 9

Issue:

Appears on pages(s): 35-63

Keywords:

DOI: 10.14359/17219

Date: 1/1/1964

Abstract:
A hypothesis for creep is presented in terms of the microstructure and properties of hydrated cement. An experimental investigation, designed to provide a quantitative basis for the hypothesis, is briefly described. Procedures are presented for estimating creep in terms of the volumetric composition of the concrete, the degree of hydration, and the observed free shrinkage characteristics.