In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
Staff Directory
ACI World Headquarters 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA Phone: 1.248.848.3800 Fax: 1.248.848.3701
ACI Middle East Regional Office Second Floor, Office #207 The Offices 2 Building, One Central Dubai World Trade Center Complex Dubai, UAE Phone: +971.4.516.3208 & 3209
ACI Resource Center Southern California Midwest Mid Atlantic
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: Tests on Slender Prestressed Concrete Columns
Author(s): H. R. Brown and A. S. Hall
Publication: Symposium Paper
Volume: 13
Issue:
Appears on pages(s): 179-192
Keywords:
DOI: 10.14359/16760
Date: 1/1/1966
Abstract: Reports the results of tests on 30 eccentrically loaded prestressed concrete columns with an I/t ratio of 33. The degree of prestress varied from zero to 0.6 f'c. This paper examines the effect of prestressing on the loadcarrying capacity of slender columns and questions whether an optimum degree of prestress occurs.