Strength-Increasing Effects of a Chloride-Free Accelerator

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strength-Increasing Effects of a Chloride-Free Accelerator

Author(s): Sandor Popovics

Publication: Symposium Paper

Volume: 102

Issue:

Appears on pages(s): 79-106

Keywords: accelerating agents; cement pastes; compressive strength; concretes; epoxy resins; fly ash; formates; mortars (material); portland cements; Materials Research

DOI: 10.14359/1620

Date: 9/1/1987

Abstract:
Strength-increasing effects of achloride-free accelerating admixture are investigated on various portland cement pastes, mortars and concretes with or without other admixtures. Although the test results are preliminary in nature, the available experimental evidence shows that this chloride-free accelerator increases significantly the strengths of a wide variety of cementitious compositions including portland cement, epoxy, pozzolans and combinations of these.