Title:
Proposed Revised Specifications for Conrete Sidewalks
Author(s):
ACI Committee on Sidewalks and Floors
Publication:
Journal Proceedings
Volume:
13
Issue:
2
Appears on pages(s):
351-357
Keywords:
none
DOI:
10.14359/15895
Date:
2/1/1917
Abstract:
These specifications apply to concrete sidewalks in residence and business districts, and cover the preparation of the sub-base, the laying and finishing of the walk and its protection during early hardening.