Title: Architectural Design of the Concrete House
Author(s): E.G. Perrot
Publication: Journal Proceedings
Volume: 14
Issue: 6
Appears on pages(s): 416-418
Keywords: none
DOI: 10.14359/15816
Date: 6/1/1918
Abstract: With the growing importance of the necessity for permanent construction of good homes for the wage-earner is the all important one of materials for construction coupled with successful architectural design.