Title: Reinforced-Concrete Flat-Slab Railway Bridges
Author(s): A.B. Cohen
Publication: Journal Proceedings
Volume: 14
Issue: 6
Appears on pages(s): 321-334
Keywords: none
DOI: 10.14359/15805
Date: 6/1/1918
Abstract: The art of reinforced concrete had its inception in Europe and flourished there for a number of years before taking root in this country.