Title: The Economic Possibilities of Lightweight Aggregate in Building Construction

Author(s): A.W. Stephens

Publication: Journal Proceedings

Volume: 16

Issue: 2

Appears on pages(s): 152-155

Keywords: none

DOI: 10.14359/15742

Date: 2/1/1920

Abstract:
For the construction of reinforced-concrete ships it was desirable to develop a concrete of minimum weigth and maximum strength. This was accomplished by the use of a special fine ground portland cement and an aggregate which has been described in the technical press as "an artifically burned clay or shale uniformly filled with small non-connecting cells." This concrete weighed about 115 lb. per cu. Ft.; the mixture being one part cement, two-thirds part fine aggregate, and one and one-third parts coarse aggregate.




  

Edit Module Settings to define Page Content Reviewer