Title: Inundation Methods for Measurements of Sand in Making Concrete
Author(s): G.A. Smith and W.A. Slater
Publication: Journal Proceedings
Volume: 19
Issue: 1
Appears on pages(s): 222-240
Keywords: none
DOI: 10.14359/15649
Date: 1/1/1923
Abstract: It is with the purpose of developing the principles of a proposed method of accurate field measurement of sand and of water for concrete that the investigation reported in this paper was undertaken.