Title: Fire Resistance of Concrete Building Units

Author(s): ACI Committee P-5

Publication: Journal Proceedings

Volume: 21

Issue: 2

Appears on pages(s): 528-536

Keywords: none

DOI: 10.14359/15540

Date: 2/1/1925

Abstract:
During 1924, your committee has completed its study and review of the tests carried out at the Underwriter's Laboratories and has received from the laboratories its report and copy of their recommendations based thereon. These recommendations have been submitted to the fire council of the Underwriter's Laboratories and approved by them.




  