International Concrete Abstracts Portal

  


Title: Concrete Pavement Design

Author(s): L.W. Teller and J.T. Pauls

Publication: Journal Proceedings

Volume: 22

Issue: 2

Appears on pages(s): 314-347

Keywords: none

DOI: 10.14359/15451

Date: 2/1/1926

Abstract:
One of the most outstanding developments in this country during the past few years has been the phenomenal growth of motor transportation. The production of low cost motor equipment and cheap motor fuel have created a demand for improved highways. The highway engineer has been faced with the urgent necessity for the design, construction and maintence of a sufficient mileage of highway, of a type best suited to the conditions of location, traffic and funds available.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer