Title: Effect of Temperature on the Curing of Concrete

Author(s): R.A. Foley

Publication: Journal Proceedings

Volume: 25

Issue: 2

Appears on pages(s): 566-572

Keywords: none

DOI: 10.14359/15355

Date: 2/1/1929

Abstract:
Conrete of various classifications is being used more and more in all seasons, irrespective of temperature or climatic conditions. It is of special economic importance to manufactures of concrete products as well as to the contractors and engineers responsible for the design and construction of concrete structures to be properly informed as to the effect of temperature on the strength of concrete.




  