Title:
SP-013: Symposium on Reinforced Concrete Columns
Author(s):
Editor: Boris Bresler
Publication:
Symposium Paper
Volume:
13
Issue:
Appears on pages(s):
378
Keywords:
DOI:
10.14359/14065
Date:
1/1/1966
Abstract:
SP13
Selected papers dealing with experimental and analytical studies of reinforced and prestressed concrete columns, are contained in this volume. Compilation of the papers has been carried out under the sponsorship of the joint ACI-ASCE Committee 441, Reinforced Concrete Columns, in accordance with the committee’s three main objectives: (I) to review and correlate information on the analysis and design of concrete columns, including the methods required by various building codes; (2) to encourage experimental research on column behavior; (3) to propose design criteria for concrete columns.