Abstract:
A study was made of why a 35-year-old bridge slab subjected to deicing salts was in pristine condition. When demolished, the post-tensioned cast-in-place Connecticut bridge consisting of fourteen 120 ft (37 m) spans was found free of rebar corrosion and delaminations. Tests performed on salvaged slab specimens showed that chloride ingress was lower than it was for usual concretes. The slab behaved similar to a low water-cement ratio silica fume concrete. The excellent behavior is attributed to low water-cement ratio; high cement content; minimum cracking; well-graded fine aggregate; a high dosage of water reducer/retarder; good consolidation; good curing; good concrete cover-to-reinforcement; longitudinal compression in the slab applied 3 days after casting; and the stiffness of the superstructure.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer