Title: Inspection of Building Construction

Author(s): Leonard E. Dunlap

Publication: Journal Proceedings

Volume: 46

Issue: 4

Appears on pages(s): 609-612

Keywords: no keywords

DOI: 10.14359/12078

Date: 4/1/1950

Abstract:
From the viewpoint of an architect, inspection on a job involving architectural and structural concrete encompasses a number of factors. Accurate plans and specifications, testing and developing the concrete mix design, proper erection of forms and placement of concrete, and systematic curing require close attention by a competent superintendent and qualified inspectors.




  