Abstract:
Vacumn concrete processes were introduced in this country a number of years ago and their applications in building construction have been reported in he ACI Journal. During the last few years these processes have become known and adopted in many foreign countries particularly in Europe, and this paper deals with these foreign developments, singling out new ways and methods in construction.