Proposed Revision of ACI 614-59: Reccomended Practice for Measuring, Mixing, and Placing Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Revision of ACI 614-59: Reccomended Practice for Measuring, Mixing, and Placing Concrete

Author(s): ACI Committee 304

Publication: Journal Proceedings

Volume: 69

Issue: 7

Appears on pages(s): 374-414

Keywords: admixtures; aggregate gradation; aggregates; air entrainment; batching; cement content; cement storage; coarse aggregates; concrete construction; concrete finishing (fresh concrete); concretes; consolidation; construction joints; conveying; conveyors.

DOI: 10.14359/11272

Date: 7/1/1972

Abstract:
Presents recommended methods and procedures for measuring, mixing, trans-porting, and placing concrete. Best practices are described rather than common practices; thus, the recommendations are made on a "should" basis leaving to the user the responsibility of placing them on a "shall" basis in specifications for a particular job. Although many of the recommendations made can be used in connection with special concretes, it is normal weight concrete to which they principally apply. Among the topics covered are: control, handling, and storage of materials, in-cluding pozzolans and admixtures; measurement of constituent materials; measuring equipment; batching tolerances; mixing, including ready-mixed concrete; retempering of mixes; mixing time; and mixers. Methods of placing such as hoppers, buckets, buggies, belt conveyors, chutes, and drop pipes are covered. Paving equipment is also discussed. Sections are devoted to the special areas of: transporting concrete in revolving drum mixers; transporting centrally-mixed concrete; preplaced aggregate concrete; tremie concrete and equipment; equipment and proportioning for pumping concrete; forms; cleanup and joint preparation; and finishing unformed surfaces. An extensive list of references is given.