International Concrete Abstracts Portal

  


Title: Bleeding in Concrete- A Microscopic Study

Author(s): John E. Ash

Publication: Journal Proceedings

Volume: 69

Issue: 4

Appears on pages(s): 209-211

Keywords: anisotropy;bleeding (concrete);concretes;deformation;durablity; microcracking; microscopy;microstructure;research;tensile strength;tension tests.

DOI: 10.14359/11264

Date: 4/1/1972

Abstract:
Bleeding can have far-reaching effects on the preparation of concrete and it’s a phenomenon which has too often been ignored. This paper briefly discusses some of its important consequences with particular emphasis on tensile strength and deformational behavior, and suggests a method by which effects of bleeding on the internal structure of concrete may be studied.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.