Title: Nonlinear Concrete Wall Characteristics of Significant Importance in Structural Analysis

Author(s): F . Bljuger

Publication: Journal Proceedings

Volume: 75

Issue: 6

Appears on pages(s): 244-250

Keywords: bearing capacity; bearing walls: bending moments;deformation; joints (junctions) ; modulus of elasticity;multistory buildings; plastic analysis; precast concrete; strains;stress-strain relationships; structural analysis; walls.

DOI: 10.14359/10937

Date: 6/1/1978

Abstract:
Dominant structural features of precast walls in concrete buildings, and their influence on the non-linear characteristics of the latter, are considered. The analysis takes into account local plastic deformation of the failure zones and the strain property of the wall at a decrease of stresses. Methods are proposed for evaluation of ultimate bending moments and curvatures at the Iimit state.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer