International Concrete Abstracts Portal

  


Title: Ring Fiber Reinforced Concrete

Author(s): Andrew H. Stages and John Minor

Publication: Journal Proceedings

Volume: 78

Issue: 5

Appears on pages(s): 369-373

Keywords: bond (concrete to reinforcement); fiber reinforced concretes; metal fibers; strength; tests.

DOI: 10.14359/10521

Date: 9/1/1981

Abstract:
This experimental program was a study of the bonding behavior of small 1’4 in. (32 mm) diameter discrete, continuous steel rings randomly distributed in a concrete matrix and of the strength-increasing potential they offer as reinforcement. Advantages of ring shape versus straight fibers are discussed. Bending, compression, and splitting tension tests indicate the rings at the concentrations tested are superior to straight fiber reinforcement in some respects. Possible refinements of the ring reinforcement technique are discussed.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer