207.5R-99: Roller-Compacted Mass Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 207.5R-99: Roller-Compacted Mass Concrete

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 47

Keywords: admixtures; aggregates; air entrainment; compacting; compressive strength; concrete; conveying; creep properties; curing; joints (junctions); mixture proportioning; placing; shear properties; vibration; workability.

DOI:

Date: 3/29/1999

Abstract:

Note: A newer version of this document exists. This document was replaced by 207.5R-11.

Roller-compacted concrete (RCC) is a concrete of no-slump consistency in its unhardened state that is transported, placed, and compacted using earth and rockfill construction equipment. This report includes the use of RCC in structures where measures should be taken to cope with the generation of heat from hydration of the cementitious materials and attendant volume change to minimize cracking. Materials mixture proportioning, properties, design considerations, construction, and quality control are covered.