Title: Specifications for Structural Concrete for Buildings (ACI 301-72)

Author(s): ACI Committee 301

Publication: Journal Proceedings

Volume: 69

Issue: 7

Appears on pages(s): 373

Keywords: Specifications for structural concrete for buildings,

Date: 7/1/1972

Abstract:
Announced adoption as standard by letter ballot May 15, 1972 of specification as reference standard for engineer or architect. Document covers materials, proportioning of concrete, reinforcing, prestressing steels, production, placing, curing, repair of surface defects, finishing, and includes provisions governing testing, evaluation and acceptance.




  