Title:
Synergistic Nano -CaCO3-PDA Modified PVA Fiber-Reinforced Concrete for Lined Rock Caverns (Prepublished)
Author(s):
Yitao Zhou, Guibin Wang, Huandui Liu, Yu Song, Mida Fang
Publication:
Materials Journal
Volume:
Issue:
Appears on pages(s):
Keywords:
high ductility concrete; interfacial transition zone; lined rock caverns; nano-CaCO3; polydopamine
DOI:
10.14359/51752078
Date:
9/23/2026
Abstract:
Lined rock cavern (LRC) hydrogen storage requires concrete linings with high tensile ductility and stable crack-control capacity under circumferential tension. Although polyvinyl alcohol (PVA) fibers exhibit high tensile strength and good alkali resistance, their hydrophilicity may induce a loose interfacial transition zone (ITZ), thereby limiting effective fiber bridging. This study proposes a cost-effective fiber-surface modification strategy by combining polydopamine (PDA) with nano-CaCO3. Unlike conventional single surface-treatment methods, the proposed system simultaneously introduces a protective slip-buffering layer and a mineral particle-enhanced ITZ. The PDA layer serves as an adhesive carrier and a protective slip layer, reducing direct abrasion between the fiber and cementitious matrix during interfacial sliding. Meanwhile, nano-CaCO3 particles anchored on the PDA layer increase fiber-surface roughness and provide nucleation/filling sites for hydration products, promoting ITZ densification and stronger mechanical interlocking. SEM and FTIR results confirm the successful formation of the PDA/nano-CaCO3 coating, while tensile tests and DIC analysis show that the modified fibers promote stable strain hardening and more uniform multiple cracking. Numerical simulation further indicates that the improved HDC lining can disperse localized cracking and alleviate damage transfer to the surrounding rock. These results demonstrate that the PDA-assisted nano-CaCO3 modification provides an effective physicochemical route for enhancing PVA fiber-reinforced HDC used in LRC hydrogen storage.