Modeling Parameters and Acceptance Criteria for RC Walls: Phase III – Diagonal Shear-Controlled Walls (Prepublished)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modeling Parameters and Acceptance Criteria for RC Walls: Phase III – Diagonal Shear-Controlled Walls (Prepublished)

Author(s): Saman A. Abdullah, John W. Wallace, Wassim M. Ghannoum, Mohamed M. Talaat, Garrett Hagen, and Laura Lowes

Publication: Structural Journal

Volume:

Issue:

Appears on pages(s):

Keywords: acceptance criteria; concrete walls; modeling parameters; retrofit; seismic evaluation; shear-controlled

DOI: 10.14359/51752072

Date: 9/17/2026

Abstract:
Most of the provisions for concrete structural walls in ASCE/SEI 41-17 were developed in the late 1990s based on limited experimental data and judgment for FEMA-273 (1997a) and FEMA-274 (1997b). The only exception being the modeling parameters and acceptance criteria of shear-controlled walls, which were updated for ASCE/SEI 41-06 Supplement 1 (Elwood et al., 2007). As a result, the wall provisions tend to be, in many cases, inaccurate and conservative, and thus can produce uneconomical retrofit schemes. This study involves utilizing available experimental data from a large wall test database (more than 1,100 wall tests) and new information on the performance of structural walls to develop modeling parameters and acceptance criteria for diagonal shear-controlled walls that will produce improved seismic assessments of wall buildings. Assessment outcomes between the provisions of ASCE/SEI 41-17 and the proposed provisions showed that the current provisions in ASCE/SEI 41-17 are, in many cases, overly conservative for many structures.