Title:
Study On Mechanical Properties and Microscopic Mechanism of Bio-Inspired Geopolymer Cementitious Materials (Prepublished)
Author(s):
Zhixin Wang, Zihao Wu, Yueyue Feng, Hui Ma, Qingtao Zhang
Publication:
Materials Journal
Volume:
Issue:
Appears on pages(s):
Keywords:
bio-inspired solution; geopolymer cementitious material; mechanical properties; microstructure; polyreaction
DOI:
10.14359/51752070
Date:
9/16/2026
Abstract:
As a green cementitious material, geopolymers exhibit inherent limitations in engineering applications, such as an underdeveloped microstructure and a weak interfacial transition zone (ITZ). In order to solve these problems, this paper is inspired by the mechanism of anion and cation action in desert sand worm secretion and prepares a bio-inspired modifier to realize the regulation of the microstructure and mechanical properties of geopolymer cementitious materials. In this study, a bio-inspired modification strategy was proposed to optimize the performance of slag-silica fume-based geopolymer. The bio-inspired solution prepared by sodium alginate ( SA ), quaternized chitosan ( QC ) and silane coupling agent ( SCA ) through a specific process was used as a modifier to obtain an inorganic-organic composite system-bio-inspired geopolymer cementitious material ( BGCM ). The microscopic modification mechanism of BGCM was thoroughly investigated by determining its unconfined compressive strength (UCS) and integrating multiple characterization techniques, including X-ray diffraction (XRD), Fourier-transform infrared spectroscopy (FTIR), scanning electron microscopy-energy-dispersive spectroscopy (SEM-EDS), and Brunauer-Emmett-Teller (BET) specific surface area and pore size analysis. The results indicate that when the bio-inspired solution content is 9 wt.%, the 7-day cured BGCM exhibits a 16% increase in UCS compared to the reference specimen (without bio-inspired solution), while the 28-day UCS is enhanced by 14%. Concurrently, the single-point BET specific surface area is reduced by 18%. In the FTIR spectra, the characteristic Si–O–T (T=Si, Al) stretching band at 900–1200 cm⁻¹, a typical indicator of geopolymerization, becomes narrower and more intense.