Title:
Evolution of Strength and Shrinkage of Ground Granulated Blast Furnace Slag-Based Ambient-Cured Alkali-Activated Reactive Powder Concrete Incorporating Reactive MgO (Prepublished)
Author(s):
Md Mamun Hossain, M. Neaz Sheikh, and Muhammad N.S. Hadi
Publication:
Materials Journal
Volume:
Issue:
Appears on pages(s):
Keywords:
alkali-activated reactive powder concrete; microstructure; reactive MgO; shrinkage; strength
DOI:
10.14359/51752068
Date:
9/16/2026
Abstract:
This study investigated the evolution of strength and drying shrinkage together with microstructural properties of ground granulated blast furnace slag (GGBFS)-based ambient-cured alkali-activated reactive powder concrete (AARPC) incorporating reactive MgO. The AARPC is fundamentally characterized by its very high binder content, low water-to-binder ratio, and dense particle packing, which alter hydration reactions and shrinkage behavior compared to typical alkali-activated concretes. Six AARPC mixtures incorporating 0 to 15% reactive MgO were tested for compressive and flexural strength development up to 120 days and drying shrinkage up to 56 days. Microstructural investigations, including X-ray diffraction (XRD), thermogravimetric analysis (TGA), Fourier transform infrared spectroscopy (FTIR), and scanning electron microscopy (SEM) with energy-dispersive spectroscopy (EDS), were conducted to identify hydration products and clarify phase evolution. Results showed that the addition of 5% reactive MgO led to a 6.5% improvement in compressive strength and a 32.8% increase in flexural strength at 28 days, while significantly reducing drying shrinkage through pore refinement and matrix densification. However, Higher reactive MgO contents reduced shrinkage but caused strength loss due to excessive hydrotalcite formation and microcracking. Overall, this study clarifies the mechanism by which reactive MgO influences strength and shrinkage in ambient-cured AARPC and highlights its potential for the development of cement-free, high-performance alkali-activated reactive powder concrete under ambient curing conditions.