Title:
Experimental Study of Corrosion-Induced Cracking in Reinforced Concrete Under Chloride Exposure (Prepublished)
Author(s):
Sher Khan, Muhammad Masood Rafi
Publication:
Materials Journal
Volume:
Issue:
Appears on pages(s):
Keywords:
bar diameter; chloride-induced corrosion; concrete cover cracking; corrosion-induced cracking; corrosion level; reinforced concrete durability; reinforcement corrosion; service-life prediction
DOI:
10.14359/51752067
Date:
9/16/2026
Abstract:
This study investigates corrosion-induced cracking in reinforced concrete subjected to accelerated chloride exposure, with emphasis on the applicability of Faraday’s law for predicting steel mass loss (ML). Voltage drop variation proved to be a reliable indicator of crack initiation, showing close agreement with observed surface cracking. Reduced porosity and higher electrical resistivity in low water-cement ratio (w/c) concretes restricted ionic transport, resulting in an actual corrosion level (CL) of nearly 40% of that predicted by Faraday’s law. Faraday’s law accurately estimated ML for specimens preconditioned for 28 days and cast with medium-to-high w/c, whereas shorter preconditioning durations and low w/c resulted in systematic overestimation. Concrete compressive strength, rebar diameter, w/c, concrete cover, and exposure conditions exhibited strong coupled effects on crack initiation and propagation, with crack growth rates ranging from 0.142 to 0.586 mm (0.006 to 0.023 in.) per 3% CL, highlighting the need for integrated consideration of material and geometric parameters in durability-based design and corrosion assessment. An analytical model for estimating CL at crack initiation is proposed that shows strong agreement with experimental observations.