Title:
Prediction of Elastic Modulus in Bentonite-Clay-Based Concrete Using Machine Learning (Prepublished)
Author(s):
Jinpeng Dai, Fanghui Lu, Xuwei Dong, Jieyu Zhou
Publication:
Materials Journal
Volume:
Issue:
Appears on pages(s):
Keywords:
elastic modulus; machine learning; mixture proportion optimization; sustainable concrete
DOI:
10.14359/51752066
Date:
9/16/2026
Abstract:
The elastic modulus is crucial for concrete structural design. This study develops a machine learning approach to predict the elastic modulus of bentonite-clay concrete and optimize its mixture proportions. Using a dataset containing key parameters, including cement, bentonite, and clay, the CatBoost prediction model was tuned by the Grey Wolf Optimizer and Sparrow Search Algorithm. SHAP analysis revealed the degree of influence of various material parameters on the elastic modulus and identified optimal ranges for key parameters (bentonite: 80 to 175 kg/m³; clay: 130 to 260 kg/m³). Monte Carlo simulation enabled mixture proportion optimization targeting cost minimization, achieving a modest 5.2% cost reduction as a proof‑of‑concept while meeting the target elastic modulus. This data-driven method demonstrates a proof-of-concept framework for intelligent design of bentonite-clay concrete, but its predictive model requires external validation before engineering use.