Reviving Ancient Materials: Cocciopesto’s Role in Sustainable and Durable Modern Concrete (Prepublished)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reviving Ancient Materials: Cocciopesto’s Role in Sustainable and Durable Modern Concrete (Prepublished)

Author(s): Irene Rocca, Anna Saetta, Renato Vitaliani

Publication: Materials Journal

Volume:

Issue:

Appears on pages(s):

Keywords: cocciopesto; durable concrete; massive structure; self-healing concrete; sustainable concrete

DOI: 10.14359/51752065

Date: 9/16/2026

Abstract:
This study investigates the potential of cocciopesto—a material historically used in ancient Roman constructions—to enhance the performance and sustainability of modern concrete. A dedicated experimental procedure was developed to evaluate two innovative mixture designs, obtained by partially replacing cement and sand with cocciopesto, intended respectively for large-scale massive and non-massive structural applications. The experimental program includes compressive, tensile, and flexural strength tests aimed at assessing the recovery of mechanical properties after alternating curing phases in air and water. The first experimental campaign focused on massive large-scale constructions, exploring three different mixture designs by varying the proportion of cocciopesto and lime. The most promising composition was then selected for a second campaign, targeting applications that require higher cement contents and improved early-age mechanical performance. Test results show in both cases that cocciopesto-infused concrete can retain mechanical strength and exhibit self-healing behavior in terms of mechanical strength recovery, potentially improving resistance to environmental stressors and contributing to extending the service life of concrete structures. Overall, the findings suggest that cocciopesto may represent a promising component for eco-efficient concrete, aligning with modern sustainability goals. The observed trends in mechanical recovery and long-term strength development provide a basis for further investigations into the role of cocciopesto in modern cementitious systems.