Title: Numerical Calibration of Local Bond-Slip Models (Prepublished)

Author(s): Farah Dameh and Stavroula J. Pantazopoulou

Publication: Structural Journal

Volume:

Issue:

Appears on pages(s):

Keywords: bond models; bond-slip laws; confinement index; cover to bar diameter ratio; development length; large diameter bars; size effect on bond

DOI: 10.14359/51752063

Date: 9/16/2026

Abstract:
A detailed nonlinear finite element (FE) model of the ribbed profile of reinforcement is used to investigate the effects of bar size, bonded length, confinement, and cover-to-bar ratio on the characteristics of local bond strength-slip laws and the type of anticipated bond failure. The ribbed bar model is verified first against experimental results from direct tension pullout tests, and then it is used to investigate and corroborate the parametric behavior of the model with the evidence provided by the experimental database compiled by ACI Committee 408, Bond and Development of Steel Reinforcement. The objective of the study is to extend the bond-slip laws used in FE simulations of concrete structures by accounting for important design variables that affect bond behavior, with particular emphasis on the effects of large bar diameters and confinement. The detailed ribbed bar model is further used to investigate the upper limit of the confinement index, (Ktr+C)/Db, which is set at 2.5 in ACI CODE-318-25, and marks the transition from bond splitting failure to pullout failure.