Title:
Stability of Slender GFRP-RC Columns under Various Load Eccentricities (Prepublished)
Author(s):
Basel H. Aljada and Ehab F. El-Salakawy
Publication:
Structural Journal
Volume:
Issue:
Appears on pages(s):
Keywords:
buckling; glass fiber-reinforced polymers; slender columns; stability failure
DOI:
10.14359/51752061
Date:
9/16/2026
Abstract:
Slender columns are highly susceptible to buckling, which induces additional bending moments and reduces their axial load capacity compared to short columns, potentially leading to stability failure. This study presents the results of 10 full-scale glass fiber-reinforced polymer-reinforced concrete columns with a slenderness ratio of 45, exploring the influence of longitudinal reinforcement ratio (1.21 or 3.44%) and eccentricity-to-diameter ratio (e/D = 0, 8.5, 17, or 34%). Reference specimens with slenderness ratios of 20 and 28 were included for comparison. Results revealed that the e/D ratio had the most significant influence, markedly reducing axial capacity and magnifying secondary moments. A threshold ofe/D = 17% was identified beyond which stability failure occurred. The contribution of reinforcement ratio became more apparent as the e/D ratio increased. Increasing the slenderness ratio from 20 to 28 reduced the axial capacity, while a further increase to 45 primarily increased secondary moments without a noticeable additional reduction in axial capacity.