Title:
Enhanced Machine Learning For 3D-Printed Concrete Compressive Strength (Prepublished)
Author(s):
Paul Isu, Faisal Mukhtar, and M.Z. Naser
Publication:
Materials Journal
Volume:
Issue:
Appears on pages(s):
Keywords:
3D-printed concrete; compressive strength; interpretability; machine-learning; manufacturing parameters; sustainability
DOI:
10.14359/51752060
Date:
9/16/2026
Abstract:
This paper presents a machine learning model for performance prediction of 3D-printed concrete (3DPC), which uses 37 features (the highest at the time of this research), including the material mixture composition and printing parameters. Previous models relied mostly on mixture composition, without incorporating printing parameters, which may fail to explain the system’s complex mechanochemical interaction. This study used six machine learning algorithms, namely, XGBOOST, Random Forest, Support Vector Machine, Decision Tree, K-Nearest Neighbor, and Multilinear Regression, to predict the compressive strength of 3DPC. The findings indicate that XGBOOST and RF showed superior performance, with R², RMSE, and MAE values of 0.972, 4.78 MPa, and 3.36 MPa for XGBOOST and 0.960, 5.73 MPa, and 3.89 MPa for RF. SHAP analysis showed superplasticizer, nozzle diameter, and age of specimen as the most important parameters. The XGBOOST’s 97% accuracy offers a tool for practical material optimization by reducing trial-and-error plaguing 3DPC mixture design.