Title: Novel Impulse-Response Test Method for the Condition Assessment of RC Plates (Prepublished)

Author(s): Sikandar Hayat Sajid, Luc Chouinard, Nicholas Carino

Publication: Materials Journal

Volume:

Issue:

Appears on pages(s):

Keywords: condition assessment, delamination, honeycomb, rebound hammer, reinforced concrete slab, stress-wave method

DOI: 10.14359/51752059

Date: 9/16/2026

Abstract:
A modification to the stress-wave propagation test known as impulse-response is proposed. The basic strategy of the proposed method is to apply consistent input energy by impact at set locations within the frequency range of stationary waves to obtain the vibrational response. The responses in the form of vibration time histories are transformed into the frequency domain and used with a discriminant analysis tool to identify test locations with higher responses attributed to lower energy absorption due to the presence of subsurface defects. To validate this approach, a rebound hammer, having consistent input energy, is used as an impactor rather than an instrumented hammer. Tests were performed on reinforced concrete slab specimens with and without simulated defects. Principal component analysis was performed on the covariance matrix of the amplitude spectra of responses at all test points. Factor scores based on principal components guided by the scree plot are found to be efficient in detecting debonding, delamination at two different depths, and honeycombing in the plate with defects. The proposed procedure is shown to have comparable accuracy to ultrasonic-echo shear-wave testing.