Development of a Uniaxial Material Wrapper for Creep and Shrinkage (Prepublished)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development of a Uniaxial Material Wrapper for Creep and Shrinkage (Prepublished)

Author(s): Javad Esmaeelpour, Mark D. Denavit, and Michael H. Scott

Publication: Structural Journal

Volume:

Issue:

Appears on pages(s):

Keywords: creep; numerical modeling; shrinkage; slender columns

DOI: 10.14359/51752058

Date: 9/16/2026

Abstract:
Creep and shrinkage affect a range of design considerations, from serviceability to the stability of slender reinforced concrete columns. Yet most structural engineering software lacks the tools to integrate these time-dependent effects into concrete constitutive models. To address this limitation, CreepShrinkageACI209 was developed as a modular uniaxial material wrapper and implemented in OpenSees. This wrapper superimposes creep and shrinkage strains calculated per ACI 209.2R-08 onto any user-selected base concrete constitutive model. Its modular architecture separates time-dependent effects from mechanical behavior, allowing users to add creep and shrinkage capabilities to existing material models without altering the underlying code. To validate its accuracy, a database of slender reinforced concrete column tests was developed, and the long-term behavior of these columns was compared against the predicted behavior using the CreepShrinkageACI209 wrapper. Comparisons showed that the wrapper accurately predicts both the evolution of time-dependent deflections and the reduction in load-carrying capacity observed in the tests, demonstrating its viability for long-term analysis of reinforced concrete structures. The implementation approach is extensible to other software, alternative creep and shrinkage models, and multi-axial concrete constitutive models.


ALSO AVAILABLE IN:

Electronic Structural Journal