Bond Performance of Thermo-Mechanically Treated Steel Reinforcing Bar in Normal Strength Concrete Under Accelerated Corrosion (Prepublished)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bond Performance of Thermo-Mechanically Treated Steel Reinforcing Bar in Normal Strength Concrete Under Accelerated Corrosion (Prepublished)

Author(s): Sher Khan, Muhammad Masood Rafi, Humberto Varum, Bruno Briseghella

Publication: Structural Journal

Volume:

Issue:

Appears on pages(s):

Keywords: beam-end test; bond behavior; bond strength; concrete cover; corroded bond; embedment length; pull-out specimen; reinforced concrete; thermo-mechanically treated reinforcing bar

DOI: 10.14359/51752056

Date: 9/16/2026

Abstract:
This study investigates the bond performance of thermo-mechanically treated (TMT) steel rebars embedded in concrete pull-out (PO) specimens, with and without accelerated corrosion, focusing on the effects of specimen geometry, water-cement ratio (w/c), and corrosion level (CL). Tests on cubical direct PO and beam-end (BE) specimens captured differing confinement and stress-transfer mechanisms. Uncorroded direct PO specimens showed ~14% higher peak bond stress (τmax) compared to BE specimens due to more uniform confinement, a difference that increased to nearly 80% under corrosion. Comparison with the literature confirmed the strong influence of confinement, bonded length, and stress distribution on peak and post-peak response. Increasing CL and bar diameter consistently reduced τmax, as corrosion-driven radial expansion generated microcracking and early splitting of the concrete cover. The effect of w/c was minimal at moderate CLs (≈3 to 5%), where corrosion damage dominated bond degradation. A simplified model is proposed to quantify τmax reduction as a function of corrosion and key geometric and mechanical parameters.