Shear Performance of Slender Steel Fiber-Reinforced Lightweight Concrete Beams: Influence of Size and Reinforcement Ratio (Prepublished)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Performance of Slender Steel Fiber-Reinforced Lightweight Concrete Beams: Influence of Size and Reinforcement Ratio (Prepublished)

Author(s): Ghassan Almasabha, Husam Abu Osba, Mohammad Al Gnimat

Publication: Structural Journal

Volume:

Issue:

Appears on pages(s):

Keywords: crack width, dowel action, lightweight concrete, shear, size effect, steel fiber-reinforced concrete

DOI: 10.14359/51752055

Date: 9/16/2026

Abstract:
Extensive research has explored the size effect on the shear capacity of reinforced concrete slender beams, yet limited studies have investigated this phenomenon in steel fiber-reinforced lightweight concrete (SFRLC) members without shear reinforcement. ACI CODE-318-19 restricts the use of deformed steel fibers as an alternative to minimum shear reinforcement to normalweight concrete members with a compressive strength not exceeding 41 MPa (6000 psi) and a member height not exceeding 610 mm (24 in.). The provision does not permit deformed steel fibers to be used as minimum shear reinforcement in lightweight concrete members, regardless of member height. This study addresses this gap by examining the size effect and the influence of longitudinal reinforcement ratios on the shear behavior of large-scale SFRLC beams. Six slender beams with effective depths of 700 mm [27.6 in.], 800 mm [31.5 in.], and 1000 mm [39.4 in.] were tested under a constant shear span-to-depth ratio (𝑎/𝑑=3.5) and longitudinal reinforcement ratios of 1% and 1.5%. Hooked-end steel fibers were added at 0.5% of the concrete volume to evaluate their contribution to shear capacity. The results revealed that the experimental shear stresses at failure loading decreased as the effective depth increased, confirming the size effect in SFRLC beams. Beams with a longitudinal reinforcement ratio of 1.5% exhibited significantly higher shear capacities than those with a 1.0% reinforcement ratio, with increases of approximately 52.8%, 23.4%, and 39.0% for effective depths of 700 mm (27.6 in.), 800 mm (31.5 in.), and 1000 mm (39.4 in.), respectively. The inclusion of steel fibers enhanced the shear capacity and provided an effective alternative to the minimum shear reinforcement specified by ACI CODE-318-19 for lightweight concrete members. This study highlights the potential of steel fibers to improve the structural performance of lightweight SFRC beams and offers insights to inform design practices for large-scale members.


ALSO AVAILABLE IN:

Electronic Structural Journal