Title:
Comparison of Post-Tensioned Slabs with Steel Fiber Reinforcement versus Conventional Bonded Reinforcement
Author(s):
Taye Ojo, Carol Hayek, Hendrik Thooft, and Carin Roberts-Wollmann
Publication:
Structural Journal
Volume:
123
Issue:
5
Appears on pages(s):
289-302
Keywords:
banded-banded; bonded; flat plate; post-tensioned; prestressed; slab; steel fibers; tendon; unbonded; uniform-banded
DOI:
10.14359/51751798
Date:
9/1/2026
Abstract:
This paper compares the flexural performance of post-tensioned slabs with steel fiber reinforcement to post-tensioned slabs with conventional bonded reinforcement in terms of behavior at service and factored loads and flexural strength. A total of five one-third -scale models of a two-way post-tensioned flat plate were tested under uniformly distributed loads. All slabs had the same dimensions and were designed to meet allowable stresses per ACI CODE-318. The specimens varied with respect to the post-tensioning tendon layouts (banded-uniform versus banded-banded), post-tensioning type (unbonded versus bonded), and nonprestressed reinforcement (conventional bonded reinforcement versus distributed steel fibers).
Each nine-bay specimen was loaded to service and factored load multiple times, then loaded to failure. The performances of all specimens were very similar at service and factored loads. All specimens with unbonded tendons achieved similar failure loads, while the specimens with bonded post-tensioning tendons achieved a considerably higher load at failure.
Related References:
1. Kosut, G. M.; Burns, N. H.; and Winter, C. V., “Test of Four-Panel Post-Tensioned Flat Plate,” Journal of Structural Engineering, ASCE, V. 111, No. 9, 1985, pp. 1916-1929. doi: 10.1061/(ASCE)0733-9445(1985)111:9(1916)
2. ACI Committee 318, “Building Code Requirements for Reinforced Concrete (ACI 318-77),” American Concrete Institute, Farmington Hills, MI, 1977, 103 pp.
3. ACI Committee 318, “Building Code for Structural Concrete—Code Requirements and Commentary (ACI CODE-318-25),” American Concrete Institute, Farmington Hills, MI, 2025, 702 pp.
4. Joint ACI-PTI Committee 320, “Post-Tensioned Structural Concrete—Code Requirements and Commentary (ACI/PTI CODE-320-25),” American Concrete Institute, Farmington Hills, MI, 2025, 168 pp.
5. Hayek, C., and Thooft, H., “Innovative Concrete Slab Solution for Building Sustainable Structures,” Proceedings of the 6th fib International Congress, Oslo, Norway, 2022, pp. 2509-2517.
6. ACI Committee 360, “Guide to Design of Slabs-on-Ground (ACI 360-10),” American Concrete Institute, Farmington Hills, MI, 2010, 72 pp.
7. Edvardsen, C., “The Consultant’s View on Service Life Design,” RILEM Proceedings, Second International Symposium on Service Life Design for Infrastructures, Delft, the Netherlands, 2010, pp. 249-264
8. Ojo, T., and Roberts-Wollmann, C., “Comparison of Post-Tensioned Slabs with Banded-Uniform and Banded-Banded Tendon Arrangements,” ACI Structural Journal, V. 119, No. 4, 2022, pp. 211-224. doi: 10.14359/51734493
9. Burns, N. H., and Hemakom, R., “Test of Scale Model Post-Tensioned Flat Plate,” Journal of the Structural Division, ASCE, V. 103, No. 6, 1977, pp. 1237-1255. doi: 10.1061/JSDEAG.0004650
10. PTI DC20.8-04, “Design of Post-Tensioned Slabs Using Unbonded Tendons,” third edition, Post-Tensioning Institute, Farmington Hills, MI, 2004, 82 pp.
11. IAPMO, “Evaluation Report 664: SigmaSlab® – Dramix® Steel Fibers and CCL Post-Tensioning Materials in Concrete Slab Systems,” International Association of Plumbing and Mechanical Officials, Ontario, CA, 2022.
12. Ojo, T., “Performance of Steel Fiber Reinforced and Conventionally Reinforced Post-Tensioned Flat Plates,” PhD dissertation, Virginia Polytechnic Institute and State University, Blacksburg, VA, 2021.
13. International Code Council, “International Building Code,” Country Club Hills, IL, 2018.