Title: Splice Strengths of Widely Spaced Noncontact Splices

Author(s): Sung-Chul Chun

Publication: Structural Journal

Volume: 123

Issue: 5

Appears on pages(s): 29-40

Keywords: bond; noncontact splice; spacing; strut

DOI: 10.14359/51750681

Date: 9/1/2026

Abstract:
ACI CODE-318-25 and the fib Model Code have specified the limit of the transverse spacing of spliced bars for noncontact splices. The studies on noncontact splices show no difference in strength between the contact and noncontact splices. However, from truss analogies, load transfer between the spliced bars has been explained by compressive struts, and the effective lap length has been thought to be shorter than the splice lap length. In this study, an experimental evaluation of noncontact splices was conducted using 22 lightly reinforced slabs. A main test variable was the spacing between the spliced bars, up to 225 mm (9 in.), which is beyond the limit of ACI CODE-318-25. Inclined cracks in noncontact splices were prominent between the spliced bars and were consistent with those found in previous studies. The test results do not reveal any distinct differences in the developed bar stresses between the contact and noncontact splices. Based on the well-known hoop tensile stress model, the bottom cover was identified as the governing parameter for noncontact lap splices in lightly reinforced slabs or walls, with the effective lap length being nearly identical to the splice length. In consequence, the noncontact splice can develop the same strength as the contact splice.

Related References:

ACI Committee 318, 1971, “Building Code Requirements for Reinforced Concrete (ACI 318-71),” American Concrete Institute, Farmington Hills, MI, 78 pp.

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 520 pp.

ACI Committee 318, 2025, “Building Code for Structural Concrete—Code Requirements and Commentary (ACI CODE-318-25),” American Concrete Institute, Farmington Hills, MI, 702 pp.

ACI Committee 408, 2003, “Bond and Development of Straight Reinforcing Bars in Tension (ACI 408R-03),” American Concrete Institute, Farmington Hill, MI, 49 pp.

ACI Committee 408, 2021, “Tension Lap Splice Database,” American Concrete Institute, Farmington Hills, MI.

ASTM A615/A615M-22, 2022, “Standard Specification for Deformed and Plain Carbon-Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 8 pp.

Canbay, E., and Frosch, R. J., 2005, “Bond Strength of Lap-Spliced Bars,” ACI Structural Journal, V. 102, No. 4, July-Aug., pp. 605-614. doi: 10.14359/14565

Chamberlin, S. J., 1952, “Spacing of Spliced Bars in Tension Pull-Out Specimens,” ACI Journal Proceedings, V. 49, No. 12, Dec., pp. 261-274. doi: 10.14359/11817

Chamberlin, S. J., 1958, “Spacing of Spliced Bars in Beams,” ACI Journal Proceedings, V. 54, No. 2, Feb., pp. 689-697. doi: 10.14359/11463

Chinn, J.; Ferguson, P. M.; and Thompson, J. N., 1955, “Lapped Splices in Reinforced Concrete Beams,” ACI Journal Proceedings, V. 52, No. 10, Oct., pp. 201-213. doi: 10.14359/11597

Darwin, D.; Tholen, M. L.; Idun, E. K.; and Zuo, J., 1996, “Splice Strength of High Relative Rib Area Reinforcing Bars,” ACI Structural Journal, V. 93, No. 1, Jan.-Feb., pp. 95-107. doi: 10.14359/9680

fib, 1991, “CEB-FIP Model Code 1990: Design Code,” International Federation for Structural Concrete, Lausanne, Switzerland, 437 pp.

fib, 2024, “fib Model Code for Concrete Structures (2020),” International Federation for Structural Concrete, Lausanne, Switzerland, 780 pp.

Mun, S.-H., and Chun, S.-C., 2024, “Experiment on Noncontact Lap-Splices of D13 and D19 Reinforcing Bars with Wide Spacing between Spliced Bars,” Journal of the Korea Concrete Institute, V. 36, No. 1, Jan.-Feb., pp. 51-60. (in Korean) doi: 10.4334/JKCI.2024.36.1.051

Orangun, C. O.; Jirsa, J. O.; and Breen, J. E., 1977, “A Reevaluation of Test Data on Development Length and Splices,” ACI Journal Proceedings, V. 74, No. 3, Mar., pp. 114-122. doi: 10.14359/10993

Park, R., and Paulay, T., 1975, Reinforced Concrete Structures, John Wiley & Sons, Inc., New York, 769 pp.

Reynolds, G. C., and Beeby, A. W., 1982, “Bond Strength of Deformed Bars,” Bond in Concrete: Proceedings of the International Conference on Bond in Concrete, P. Bartos, ed., Paisley, UK, pp. 434-445.

Sagan, V. E.; Gergely, P.; and White, R. N., 1991, “Behavior and Design of Noncontact Lap Splices Subjected to Repeated Inelastic Tensile Loading,” ACI Structural Journal, V. 88, No. 4, July-Aug., pp. 420-431. doi: 10.14359/3037

Walker, W. T., 1951, “Laboratory Tests of Spaced and Tied Reinforcing Bars,” ACI Journal Proceedings, V. 47, No. 1, Jan., pp. 365-372. doi: 10.14359/11999

Zuo, J., and Darwin, D., 2000, “Splice Strength of Conventional and High Relative Rib Area Bars in Normal and High-Strength Concrete,” ACI Structural Journal, V. 97, No. 4, July-Aug., pp. 630-641. doi: 10.14359/7428


ALSO AVAILABLE IN:

Electronic Structural Journal