Title:
Comparison of Retrofitting Methods in Earthquake-Resistant Building Design with Polyurethane Brick Wall
Author(s):
Ömer Fatih Sak
Publication:
Structural Journal
Volume:
123
Issue:
5
Appears on pages(s):
131-147
Keywords:
earthquake-resistant design; polyurethane brick; seismic retrofitting; shear wall effect
DOI:
10.14359/51750674
Date:
9/1/2026
Abstract:
There is an increasing recognition of the necessity for designing structures capable of withstanding seismic activity. Two devastating earthquakes, measuring Mw 7.7 and 7.6, that struck Kahramanmaraş in February 2023 highlighted the significance of high-quality materials, adherence to building codes, and products manufactured under established standards in structures that sustained damage. Various techniques are available for reinforcing existing buildings to enhance their earthquake resilience. These methods can be classified into several categories, including column jacketing, the addition of shear walls, wrapping of columns with fiber-reinforced polymer (FRP), and the reinforcement of structures with steel components. Research on the reinforcement of existing school buildings has been carried out using a shear wall-like approach involving a newly developed polyurethane brick material, which serves as an innovative building component. To validate the material properties, experimental studies including compression and three-point bending tests were conducted on polyurethane brick samples of varying densities in accordance with ASTM standards. The existing structural framework was evaluated against new performance benchmarks in conjunction with cost assessments. Subsequently, a comparative analysis was conducted between the newly developed polyurethane brick material and traditional reinforcement techniques, which included an assessment of its potential applications in the construction industry.
Related References:
Stiffness on the Seismic Performance of Code-Conforming Reinforced Concrete Shear Wall Buildings,” Engineering Structures, V. 219, 2020, p. 110724. doi: 10.1016/j.engstruct.2020.110724
2. Tang, Y., and Zhang, J., “Probabilistic Seismic Demand Analysis of a Slender RC Shear Wall Considering Soil–Structure Interaction Effects,” Engineering Structures, V. 33, 2011, pp. 218-229. doi: 10.1016/j.engstruct.2010.10.011
3. Pečnik, J. G.; Gavrić, I.; Sebera, V.; Kržan, M.; Kwiecień, A.; Zając, B.; and Azinović, B., “Mechanical Performance of Timber Connections Made of Thick Flexible Polyurethane Adhesives,” Engineering Structures, V. 247, 2021, p. 113125. doi: 10.1016/j.engstruct.2021.113125
4. Zhou, J.; Wang, X.; Su, C.; Huang, H.; Liu, X.; and Wu, Z., “Experimental Investigation on the Fatigue Performance of Multi-Tendon Basalt Fiber Reinforced Polymer Cable,” Engineering Structures, V. 297, 2023, p. 116963. doi: 10.1016/j.engstruct.2023.116963
5. Williams, R. J.; Gardoni, P.; and Bracci, J. M., “Decision Analysis for Seismic Retrofit of Structures,” Structural Safety, V. 31, No. 2, 2009, pp. 188-196. doi: 10.1016/j.strusafe.2008.06.017
6. Pohoryles, D. A.; Maduta, C.; Bournas, D. A.; and Kouris, L. A., “Energy Performance of Existing Residential Buildings in Europe: A Novel Approach Combining Energy with Seismic Retrofitting,” Energy and Buildings, V. 223, 2020, p. 110024. doi: 10.1016/j.enbuild.2020.110024
7. Ozkul, T. A.; Kurtbeyoglu, A.; Borekci, M.; Zengin, B.; and Kocak, A., “Effect of Shear Wall on Seismic Performance of RC Frame Buildings,” Engineering Failure Analysis, V. 100, 2019, pp. 60-75. doi: 10.1016/j.engfailanal.2019.02.032
8. Sivakumar, S., and Kumar, B., “Enhancement of Bending Strength of Polyurethane Foam Reinforced with Basalt Fiber with Silica Nanoparticles in Comparison with Plain Polyurethane Foam,” Materials Today: Proceedings, V. 79, 2023, pp. 69-74. doi: 10.1016/j.matpr.2022.08.343
9. Papavasileiou, G. S., and Charmpis, D. C., “Earthquake-Resistant Buildings with Steel or Composite Columns: Comparative Assessment Using Structural Optimization,” Journal of Building Engineering, V. 27, 2020, p. 100988. doi: 10.1016/j.jobe.2019.100988
10. Sakcalı, G. B.; Öztürk, Y.; Çelik, İ. D.; and Davraz, M., “The Effect of New Generation Polyurethane Wall Block on Single Span Steel Frame Behavior,” Journal of Building Engineering, V. 48, 2022, p. 103986. doi: 10.1016/j.jobe.2021.103986
11. Cao, X.-Y.; Shen, D.; Feng, D.-C.; Wang, C.-L.; Qu, Z.; and Wu, G., “Seismic Retrofitting of Existing Frame Buildings Through Externally Attached Sub-Structures: State of the Art Review and Future Perspectives,” Journal of Building Engineering, V. 57, 2022, p. 104904. doi: 10.1016/j.jobe.2022.104904
12. Pohoryles, D. A.; Bournas, D. A.; Da Porto, F.; Caprino, A.; Santarsiero, G.; and Triantafillou, T., “Integrated Seismic and Energy Retrofitting of Existing Buildings: A State-of-the-Art Review,” Journal of Building Engineering, V. 61, 2022, p. 105274. doi: 10.1016/j.jobe.2022.105274
13. Shaqour, E. N., and Abo Alela, A. H. M., “Life Cycle Cost Reduction of a Social Housing Building By Using Polyurethane Lightweight Bricks,” International Journal of Geomate, V. 21, No. 84, 2021, pp. 2186-2990. doi: 10.21660/2021.84.j2195
14. Calledda, C.; Montisci, A.; and Porcu, M. C., “Optimal Design of Earthquake-Resistant Buildings Based on Neural Network Inversion,” Applied Sciences, V. 11, No. 10, 2021, p. 4654. doi: 10.3390/app11104654
15. Vona, M.; Flora, A.; Carlucci, E.; and Foscolo, E., “Seismic Retrofitting Resilience-Based for Strategic RC Buildings,” Buildings, V. 11, No. 3, 2021, p. 111. doi: 10.3390/buildings11030111
16. Gentile, R., and Galasso, C., “Simplified Seismic Loss Assessment for Optimal Structural Retrofit of RC Buildings,” Earthquake Spectra, V. 37, No. 1, 2021, pp. 346-365. doi: 10.1177/8755293020952441
17. Güler, K., and Celep, Z., “On the General Requirements for the Design of Earthquake Resistant Buildings in the Turkish Building Seismic Code of 2018,” Materials Science and Engineering, V. 737, 2020. doi: 10.1088/1757-899X/737/1/012015
18. Iftode, V.-I.; Olteanu-Dontov, I.; Mihai, P.; Budescu, M.; and Harja, M., “Improving Elastic Properties of Bricks by Polyurethane Matrices Mean,” Materials Science and Engineering, V. 586, No. 1, 2019, p. 012009. doi: 10.1088/1757-899X/586/1/012009
19. Anwar, G. A., and Dong, Y., “Seismic Resilience of Retrofitted RC Buildings,” Earthquake Engineering and Engineering Vibration, V. 19, No. 3, 2020, pp. 561-571. doi: 10.1007/s11803-020-0580-z
20. Alaloul, W. S.; John, V. O.; and Musarat, M. A., “Mechanical and Thermal Properties of Interlocking Bricks Utilizing Wasted Polyethylene Terephthalate,” International Journal of Concrete Structures and Materials, V. 14, No. 1, 2020, p. 24. doi: 10.1186/s40069-020-00399-9
21. Klingner, R. E., and Bertero, V. V., “Earthquake Resistance of Infilled Frames,” Journal of the Structural Division, ASCE, V. 104, No. 6, 1978, pp. 973-989.
22. Terán-Gilmore, A.; Bertero, V. V.; and Youssef, N. F. G., “Seismic Rehabilitation of Infilled Non-Ductile Frame Buildings Using Post-Tensioned Steel Braces,” Earthquake Spectra, V. 12, No. 4, 1996, pp. 863-882. doi: 10.1193/1.1585914
23. Cansız, S., “Analytical Investigation of the Measures to be Taken Against Weak Storey Irregularities,” Journal of Construction, V. 22, No. 2, 2023, pp. 407-418. doi: 10.7764/RDLC.22.2.407
24. Özsoy Özbay, A. E.; Erkek, O.; and Çeribaşı, S., “The Effect of Polypropylene, Steel, and Macro Synthetic Fibers on Mechanical Behavior of Cementitious Composites,” Journal of Construction, V. 20, No. 3, 2021, pp. 591-601. doi: 10.7764/RDLC.20.3.591
25. Erdem, R. T., and Karal, K., “Performance Evaluation and Strengthening of Reinforced Concrete Buildings,” Journal of Construction, V. 21, No. 1, 2022, pp. 53-68. doi: 10.7764/RDLC.21.1.53
26. Benaied, B.; Hemsas, M.; Benanane, A.; and Hentri, M., “Seismic Analysis of RC Building Frames with Vertical Mass and Stiffness Irregularities Using Adaptive Pushover Analysis,” Journal of Construction, V. 22, No. 3, 2023, pp. 565-580. doi: 10.7764/RDLC.22.3.597
27. Escolano Sánchez, F.; Mazariegos de la Serna, A.; Sánchez Lavín, J. R.; and Campo Yagüe, J. M., “Underpinning of Shallow Foundations by Expansive Polyurethane Resin Injections. Case study: Cardinal Diego de Espinosa Palace in Segovia Spain,” Journal of Construction, V. 16, No. 3, 2017, pp. 420-430. doi: 10.7764/RDLC.16.3.420
28. Moehle, J. P., “Earthquake-Resistant Design of Reinforced Concrete Structures: Shortcomings of Current Methods,” ACI Structural Journal, V. 100, No. 1, Jan.-Feb. 2003, pp. 11-18. doi: 10.14359/12338
29. Beyer, K.; Dazio, A.; and Priestley, M. J. N., “Shear Deformations of Slender Reinforced Concrete Walls Under Seismic Loading,” ACI Structural Journal, V. 108, No. 2, Mar.-Apr. 2012, pp. 167-177. doi: 10.14359/51684223
30. Aquino, W., and Hawkins, N. M., “Seismic Retrofitting of Corroded Reinforced Concrete Columns Using Carbon Composites,” ACI Structural Journal, V. 104, No. 3, May-June 2007, pp. 348-356. doi: 10.14359/18625
31. “Türkiye Bina Deprem Yönetmeliği,” Resmî Gazete, Ankara, Turkey, https://www.resmigazete.gov.tr/eskiler/2018/03/20180318M1-2.htm. (last accessed Sept. 6, 2026)
32. Ansys, “Ansys User’s Manual Revision 23.1,” ANSYS, Inc., Canonsburg, PA, 2023.
33. Qiu, D.; He. Y.; and Yu, Z., “Investigation on Compression Mechanical Properties of Rigid Polyurethane Foam Treated Under Random Vibration Condition: An Experimental and Numerical Simulation Study,” Materials, V. 12, No. 20, p. 3385. doi: 10.3390/ma12203385
34. Turkish Chamber of Civil Engineers, “Damage Evaluation of Reinforced Concrete and Masonry Buildings Subjected to Earthquake Loads,” Disaster Preparation and Intervention Committee, Ankara, Turkey, 2016.
35. FEMA P-58, “Seismic Performance Assessment of Buildings, Volume 1 – Methodology,” Federal Emergency Management Agency, Washington, DC, 2012.
36. De Lorenzis, L., and Teng, J. G., “Near-Surface Mounted FRP Reinforcement: An Emerging Technique for Strengthening Structures,” Composites Part B: Engineering, V. 38, No. 2, 2007, pp. 119-143. doi: 10.1016/j.compositesb.2006.08.003
37. Yao, J.; Teng, J. G.; and Chen, J. F., “Experimental Study on FRP-to-Concrete Bonded Joints,” Composites Part B: Engineering, V. 36, No. 2, 2005, pp. 99-113. doi: 10.1016/j.compositesb.2004.06.001