Surface Treatment for Recycled Plastic Aggregate in Concrete: A Review

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Surface Treatment for Recycled Plastic Aggregate in Concrete: A Review

Author(s): Seongho Han, Nima Mahmoudzadeh Vaziri, and Kamal H. Khayat

Publication: Materials Journal

Volume: 123

Issue: 2

Appears on pages(s): 81-94

Keywords: hydrophilicity; plastic aggregate concrete; plastic waste; surface treatment

DOI: 10.14359/51749270

Date: 3/1/2026

Abstract:
The use of recycled plastic aggregate in cement-based materials has emerged as a promising strategy to reduce plastic waste and promote sustainable construction. However, the inherent hydrophobicity of plastic surfaces poses a significant challenge by limiting their bonding with the cement matrix. This review critically examines five major surface treatment methods—coating, oxidation, silane, plasma, and radiation—to enhance the compatibility of recycled plastic aggregates in cementitious composites. Coating with materials such as water glass, slag powder, or acrylic resins improved compressive strength by up to 78%, depending on the coating type. Oxidation using hydrogen peroxide or calcium hypochlorite increased hydrophilicity and improved strength by approximately 10 to 30%, while excessive treatment with NaOH- hypochlorite mixtures reduced strength by up to 60%. Silane treatment significantly enhanced surface bonding, resulting in improved mechanical properties. Plasma treatment demonstrated high efficiency, reducing contact angles from ~108 to 44.0 degrees within 30 seconds. Radiation treatment using gamma rays and microwaves increased surface roughness and strength, with gamma irradiation at 100 to 200 kGy leading to substantial improvements in compressive strength and surface morphology. To the authors’ knowledge, this is the first review to systematically compare the effectiveness, mechanisms, and limitations of these surface treatments specifically for recycled plastic aggregates in cement-based materials. This review also highlights the practical challenges of scaling such treatments, including energy demand, chemical handling, and cost, and identifies future directions, such as bio-based coatings and nanomaterial functionalization. The findings provide critical insight into optimizing surface treatments to improve the mechanical performance, durability, and sustainability of concrete incorporating plastic aggregates, supporting their broader adoption in sustainable construction practices.

Related References:

1. Xu, T.; Lv, Q.; Sheng, G.; Zhang, Y.; Liu, Y.; and Shi, L., “Evolving Patterns and Drivers of Waste Plastic Trade in Key Global Economies,” Resources, Conservation and Recycling, V. 206, July 2024, Article No. 107606. doi: 10.1016/j.resconrec.2024.107606

2. Singh, A. P.; Devi, A. S.; and Sahoo, U. K., “Quantifying Plastic Waste Generation in Aizawl City, India: Waste Management and Its Impact on Human and Environmental Health,” Environmental Science and Pollution Research, V. 30, No. 49, Oct. 2023, 107390-107402. doi: 10.1007/s11356-023-27513-0

3. Faraca, G., and Astrup, T., “Plastic Waste from Recycling Centres: Characterisation and Evaluation of Plastic Recyclability,” Waste Management, V. 95, July 2019, pp. 388-398. doi: 10.1016/j.wasman.2019.06.038

4. Han, S. H.; Khayat, K. H.; Park, S.; and Yoon, J., “Machine Learning- Based Approach for Optimizing Mixture Proportion of Recycled Plastic Aggregate Concrete Considering Compressive Strength, Dry Density, and Production Cost,” Journal of Building Engineering, V. 83, Apr. 2024, Article No. 108393. doi: 10.1016/j.jobe.2023.108393

5. The World Bank, “What a Waste 2.0: A Global Snapshot of Solid Waste Management to 2050: Trends in Solid Waste Management,” World Bank Group, Washington, DC, https://datatopics.worldbank.org/what-a-waste/trends_in_solid_waste_management.html. (last accessed Feb. 13, 2026)

6. Vivekanand, A. C.; Mohapatra, S.; and Tyagi, V. K., “Microplastics in Aquatic Environment: Challenges and Perspectives,” Chemosphere, V. 282, Nov. 2021, Article No. 131151. doi: 10.1016/j.chemosphere.2021.131151

7. Chen, H. L.; Nath, T. K.; Chong, S.; Foo, V.; Gibbins, C.; and Lechner, A. M., “The Plastic Waste Problem in Malaysia: Management, Recycling and Disposal of Local and Global Plastic Waste,” SN Applied Sciences, V. 3, No. 4, Apr. 2021, Article No. 437. doi: 10.1007/s42452-021-04234-y

8. OECD, “Plastic Pollution Is Growing Relentlessly as Waste Management and Recycling Fall Short, Says OECD,” Organisation for Economic Co-operation and Development, Paris, France, Feb. 22, 2022, https://www.oecd.org/en/about/news/press-releases/2022/02/plastic-pollution-is- growing-relentlessly-as-waste-management-and-recycling-fall-short.html. (last accessed Feb. 13, 2026)

9. Canopoli, L.; Fidalgo, B.; Coulon, F.; and Wagland, S. T., “Physico- Chemical Properties of Excavated Plastic from Landfill Mining and Current Recycling Routes,” Waste Management, V. 76, June 2018, pp. 55-67. doi: 10.1016/j.wasman.2018.03.043

10. Kibria, M. G.; Masuk, N. I.; Safayet, R.; Nguyen, H. Q.; and Mourshed, M., “Plastic Waste: Challenges and Opportunities to Mitigate Pollution and Effective Management,” International Journal of Environmental Research, V. 17, No. 1, Feb. 2023, Article No. 20. doi: 10.1007/s41742-023-00507-z

11. Al-Salem, S. M.; Lettieri, P.; and Baeyens, J., “Recycling and Recovery Routes of Plastic Solid Waste (PSW): A Review,” Waste Management, V. 29, No. 10, Oct. 2009, pp. 2625-2643. doi: 10.1016/j.wasman.2009.06.004

12. Merrington, A., “Recycling of Plastics,” Applied Plastics Engineering Handbook: Processing, Sustainability, Materials, and Applications, third edition, M. Kutz, ed., William Andrew, Oxford, UK, 2023, pp. 191-217.

13. Geyer, R.; Jambeck, J. R.; and Law, K. L., “Production, Use, and Fate of All Plastics Ever Made,” Science Advances, V. 3, No. 7, July 2017, Article No. e1700782. doi: 10.1126/sciadv.1700782

14. Stina, “2019 Plastic Recycling Data,” Stina Inc., Sonoma, CA, https://circularityinaction.com/2019PlasticRecyclingData. (last accessed Feb. 13, 2026)

15. Lebreton, L.; Egger, M.; and Slat, B., “A Global Mass Budget for Positively Buoyant Macroplastic Debris in the Ocean,” Scientific Reports, V. 9, No. 1, 2019, Article No. 12922. doi: 10.1038/s41598-019-49413-5

16. Hopewell, J.; Dvorak, R.; and Kosior, E., “Plastics Recycling: Challenges and Opportunities,” Philosophical Transactions of the Royal Society B: Biological Sciences, V. 364, No. 1526, July 2009, pp. 2115-2126. doi: 10.1098/rstb.2008.0311

17. Li, H.; Aguirre-Villegas, H. A.; Allen, R. D.; Bai, X.; Benson, C. H.; Beckham, G. T.; Bradshaw, S. L.; Brown, J. L.; Brown, R. C.; Cecon, V. S.; Curley, J. B.; Curtzwiler, G. W.; Dong, S.; Gaddameedi, S.; García, J. E.; Hermans, I.; Kim, M. S.; Ma, J.; Mark, L. O.; Mavrikakis, M.; Olafasakin, O. O.; Osswald, T. A.; Papanikolaou, K. G.; Radhakrishnan, H.; Sanchez Castillo, M. A.; Sánchez-Rivera, K. L.; Tumu, K. N.; Van Lehn, R. C.; Vorst, K. L.; Wright, M. M.; Wu, J.; Zavala, V. M.; Zhou, P.; and Huber, G. W., “Expanding Plastics Recycling Technologies: Chemical Aspects, Technology Status and Challenges,” Green Chemistry, V. 24, No. 23, Dec. 2022, pp. 8899-9002. doi: 10.1039/D2GC02588D

18. Alsalami, Z. H. A.; Harith, I. K.; and Dhahir, M. K., “Utilization of Dates Palm Kernel in High Performance Concrete,” Journal of Building Engineering, V. 20, Nov. 2018, pp. 166-172. doi: 10.1016/j.jobe.2018.07.015

19. Alsalami, Z. H. A., “Study the Effect of Partially Replacement Sand by Waste Pistachio Shells in Cement Mortar,” Applied Adhesion Science, V. 5, No. 1, Dec. 2017, Article No. 19. doi: 10.1186/s40563-017-0099-3

20. Marshdi, Q. S. R.; Al-Sallami, Z. H. A.; and Zaichenko, N. M., “Effect of Multicomponent Modifier on the Properties of Cement Pastes Formulated from Self-Compacting Concrete,” Magazine of Civil Engineering, V. 98, No. 6, Oct. 2020, Article No. 9805.

21. Alsalami, Z. H. A., “Curing High-Performance Green Concrete Under Hot Weather,” Iranian Journal of Science and Technology, Transactions of Civil Engineering, V. 46, No. 1, Feb. 2022, pp. 91-99. doi: 10.1007/s40996-021-00758-w

22. Guo, Y.-C.; Li, X.-M.; Zhang, J.; and Lin, J.-X., “A Review on the Influence of Recycled Plastic Aggregate on the Engineering Properties of Concrete,” Journal of Building Engineering, V. 79, Nov. 2023, Article No. 107787. doi: 10.1016/j.jobe.2023.107787

23. Hamada, H. M.; Al-Attar, A.; Abed, F.; Beddu, S.; Humada, A. M.; Majdi, A.; Yousif, S. T.; and Thomas, B. S., “Enhancing Sustainability in Concrete Construction: A Comprehensive Review of Plastic Waste as an Aggregate Material,” Sustainable Materials and Technologies, V. 40, July 2024, Article No. e00877. doi: 10.1016/j.susmat.2024.e00877

24. Mulyadi, A.; Asrullah, A.; Anggrainy, R.; Irawan, I.; and Rizal, C., “Characteristics the Marshall Test Subsitutution of Polypropylene Plastic Pellets as Filler in Mixture Asphalt Concrete Binder Course (AC BC),” International Journal of Islamic Education, Research and Multiculturalism, V. 5, No. 2, 2023, pp. 356-375. doi: 10.47006/ijierm.v5i2.234

25. Bayiha, B. N.; Kenmogne, F.; Bahel, B.; A’Paglan Bidime, É. Y.; Bell, E. Y.; and Billong, N., “Development and Characterization of a Composite Material with Geopolymer Matrix Obtained by Incorporation of Microparticles from Plastic Bottles,” Heliyon, V. 10, No. 10, May 2024, Article No. e30801. doi: 10.1016/j.heliyon.2024.e30801

26. Borg, R. P.; Baldacchino, O.; and Ferrara, L., “Early Age Performance and Mechanical Characteristics of Recycled PET Fibre Reinforced Concrete,” Construction and Building Materials, V. 108, Apr. 2016, pp. 29-47. doi: 10.1016/j.conbuildmat.2016.01.029

27. Duan, Z.; Deng, Q.; Liang, C.; Ma, Z.; and Wu, H., “Upcycling of Recycled Plastic Fiber for Sustainable Cementitious Composites: A Critical Review and New Perspective,” Cement and Concrete Composites, V. 142, Sept. 2023, Article No. 105192. doi: 10.1016/j.cemconcomp.2023.105192

28. Almeshal, I.; Tayeh, B. A.; Alyousef, R.; Alabduljabbar, H.; Mohamed, A. M.; and Alaskar, A., “Use of Recycled Plastic as Fine Aggregate in Cementitious Composites: A Review,” Construction and Building Materials, V. 253, Aug. 2020, Article No. 119146. doi: 10.1016/j.conbuildmat.2020.119146

29. Alyousef, R.; Ahmad, W.; Ahmad, A.; Aslam, F.; Joyklad, P.; and Alabduljabbar, H., “Potential Use of Recycled Plastic and Rubber Aggregate in Cementitious Materials for Sustainable Construction: A Review,” Journal of Cleaner Production, V. 329, Dec. 2021, Article No. 129736. doi: 10.1016/j.jclepro.2021.129736

30. Alqahtani, F. K.; Sherif, M. A.; and Ghanem, A. M., “Green Lightweight Concrete Utilizing Sustainable Processed Recycled Plastic Aggregates: Technical, Economic and Environmental Assessment,” Construction and Building Materials, V. 393, Aug. 2023, Article No. 132027. doi: 10.1016/j.conbuildmat.2023.132027

31. Ogundairo, T. O.; Olukanni, D. O.; Akinwumi, I. I.; and Adegoke, D. D., “A Review on Plastic Waste as Sustainable Resource in Civil Engineering Applications,” IOP Conference Series. Materials Science and Engineering, V. 1036, No. 1, 2021, Article No. 012019. doi: 10.1088/1757-899X/1036/1/012019

32. Nyika, J., and Dinka, M., “Recycling Plastic Waste Materials for Building and Construction Materials: A Minireview,” Materials Today: Proceedings, V. 62, Part 6, 2022, pp. 3257-3262. doi: 10.1016/j.matpr.2022.04.226

33. Lamba, P.; Kaur, D. P.; Raj, S.; and Sorout, J., “Recycling/Reuse of Plastic Waste as Construction Material for Sustainable Development: A Review,” Environmental Science and Pollution Research, V. 29, No. 57, Dec. 2022, pp. 86156-86179. doi: 10.1007/s11356-021-16980-y

34. Li, X.; Ling, T.-C.; and Mo, K. H., “Functions and Impacts of Plastic/Rubber Wastes as Eco-Friendly Aggregate in Concrete – A Review,” Construction and Building Materials, V. 240, Apr. 2020, Article No. 117869. doi: 10.1016/j.conbuildmat.2019.117869

35. Barnat-Hunek, D.; Szafraniec, M.; and Pavlík, Z., “The Hydrophobization of High Strength Concretes with Plastic Waste,” AIP Conference Proceedings, V. 2305, No. 1, Nov. 2020, Article No. 020001. doi: 10.1063/5.0034027

36. Choi, Y.-W.; Moon, D.-J.; Chung, J.-S.; and Cho, S.-K., “Effects of Waste PET Bottles Aggregate on the Properties of Concrete,” Cement and Concrete Research, V. 35, No. 4, Apr. 2005, pp. 776-781. doi: 10.1016/j.cemconres.2004.05.014

37. Bágeľ, Ľ., and Matiašovský, P., “Surface Pretreatment – A Way to Effective Utilization of Waste Plastics as Concrete Aggregate. Review and First Experiences,” Proceedings of CESB10 Prague - Central Europe towards Sustainable Building: From Theory to Practice, P. Hájek, J. Tywoniak, A. Lupíšek, J. Růžička, and K. Sojková, eds., Prague, Czech Republic, 2010, 10 pp.

38. Lee, Z. H.; Paul, S. C.; Kong, S. Y.; Susilawati, S.; and Yang, X., “Modification of Waste Aggregate PET for Improving the Concrete Properties,” Advances in Civil Engineering, V. 2019, No. 1, 2019, Article No. 6942052.

39. Kaur, G., and Pavia, S., “Chemically Treated Plastic Aggregates for Eco-Friendly Cement Mortars,” Journal of Material Cycles and Waste Management, V. 23, No. 4, July 2021, pp. 1531-1543. doi: 10.1007/s10163-021-01235-2

40. Pan, Z.; Chen, J.; Zhan, Q.; Wang, S.; Jin, R.; Shamass, R.; and Rossi, F., “Mechanical Properties of PVC Concrete and Mortar Modified with Silane Coupling Agents,” Construction and Building Materials, V. 348, Sept. 2022, Article No. 128574. doi: 10.1016/j.conbuildmat.2022.128574

41. Martínez-Barrera, G.; Martínez-López, M.; del Coz-Díaz, J. J.; López-Gayarre, F.; and Varela-Guerrero, V., “Waste Polymers and Gamma Radiation on the Mechanical Improvement of Polymer Mortars: Experimental and Calculated Results,” Case Studies in Construction Materials, V. 11, Dec. 2019, Article No. e00273. doi: 10.1016/j.cscm.2019.e00273

42. Abu-Saleem, M.; Zhuge, Y.; Hassanli, R.; Ellis, M.; Rahman, M. M.; and Levett, P., “Microwave Radiation Treatment to Improve the Strength of Recycled Plastic Aggregate Concrete,” Case Studies in Construction Materials, V. 15, Dec. 2021, Article No. e00728. doi: 10.1016/j.cscm.2021.e00728

43. Lu, Z.; Yin, R.; Yao, J.; and Leung, C. K. Y., “Surface Modification of Polyethylene Fiber by Ozonation and Its Influence on the Mechanical Properties of Strain-Hardening Cementitious Composites,” Composites Part B: Engineering, V. 177, Nov. 2019, Article No. 107446. doi: 10.1016/j.compositesb.2019.107446

44. Signorini, C., and Volpini, V., “Mechanical Performance of Fiber Reinforced Cement Composites Including Fully-Recycled Plastic Fibers,” Fibers, V. 9, No. 3, Mar. 2021, Article No. 16. doi: 10.3390/fib9030016

45. Farzadnia, N., and Khayat, K. H., “Modification of Nanomaterials for Nanostructured Cement-Based Materials,” Nanotechnology for Civil Infrastructure: Innovation and Eco-efficiency of Nanostructured Cement-Based Materials, K. H. Khayat and W. Meng, eds., Elsevier, Amsterdam, the Netherlands, 2023, pp. 5-37.

46. Purnomo, H.; Pamudji, G.; and Satim, M., “Influence of Uncoated and Coated Plastic Waste Coarse Aggregates to Concrete Compressive Strength,” MATEC Web of Conferences, V. 101, 2017, Article No. 01016.

47. Ramakrishnan, A., and Jegan, J., “Surface Modified Synthetic Plastic Aggregate for Concrete – Experimental and Analytical Studies,” Materials Science (Medžiagotyra), V. 29, No. 1, 2023, pp. 104-110. doi: 10.5755/j02.ms.31124

48. Lee, J. U., and Hong, J.-Y., “Comparison of Surface Modification Methods for Improving the Compatibility of Recycled Plastic Film-Based Aggregates,” Polymers, V. 13, No. 22, Nov. 2021, Article No. 3956. doi: 10.3390/polym13223956

49. Correa, P. M.; Santana, R. M. C.; Guimarães, D.; and Graeff, A. G., “Post-Consumer PP as Partial Substitute of Sand: Effect of Surface Treatment PP with Surfactant on Concrete Properties,” Composite Interfaces, V. 27, No. 9, 2020, pp. 815-828. doi: 10.1080/09276440.2019.1702858

50. El-Nadoury, W. W., “Chemically Treated Plastic Replacing Fine Aggregate in Structural Concrete,” Frontiers in Materials, V. 9, July 2022, Article No. 948117. doi: 10.3389/fmats.2022.948117

51. Kim, K.-M., and Cho, Y.-K., “Effect of Surface Hydrophilized Plastic Waste Aggregates Made by Mixing Various Kinds of Plastic on Mechanical Properties of Mortar,” Materials, V. 17, No. 1, Jan. 2024, Article No. 247. doi: 10.3390/ma17010247

52. Naik, T. R.; Singh, S. S.; Huber, C. O.; and Brodersen, B. S., “Use of Post-Consumer Waste Plastics in Cement-Based Composites,” Cement and Concrete Research, V. 26, No. 10, Oct. 1996, pp. 1489-1492. doi: 10.1016/0008-8846(96)00135-4

53. Thorneycroft, J.; Orr, J.; Savoikar, P.; and Ball, R. J., “Performance of Structural Concrete with Recycled Plastic Waste as a Partial Replacement for Sand,” Construction and Building Materials, V. 161, Feb. 2018, pp. 63-69. doi: 10.1016/j.conbuildmat.2017.11.127

54. Zhang, Y.; Jiang, H.; Wang, H.; and Wang, C., “Separation of Hazardous Polyvinyl Chloride from Waste Plastics by Flotation Assisted with Surface Modification of Ammonium Persulfate: Process and Mechanism,” Journal of Hazardous Materials, V. 389, May 2020, Article No. 121918. doi: 10.1016/j.jhazmat.2019.121918

55. Zhang, Y.; Li, C.; Wang, L.; and Wang, H., “Application of Froth Flotation in the Separation of Polyvinyl Chloride and Polycarbonate for Recycling of Waste Plastic Based on a Novel Surface Modification,” Waste Management, V. 110, June 2020, pp. 43-52. doi: 10.1016/j.wasman.2020.05.009

56. Jiang, H.; Zhang, Y.; and Wang, H., “Surface Reactions in Selective Modification: The Prerequisite for Plastic Flotation,” Environmental Science & Technology, V. 54, No. 16, Aug. 2020, pp. 9742-9756. doi: 10.1021/acs.est.9b07861

57. Rabek, J. F., Polymer Photodegradation: Mechanisms and Experimental Methods, Springer Science+Business Media, Dordrecht, the Netherlands, 2012.

58. Liu, L.; Xu, M.; Ye, Y.; and Zhang, B., “On the Degradation of (Micro)Plastics: Degradation Methods, Influencing Factors, Environmental Impacts,” Science of the Total Environment, V. 806, Part 3, Feb. 2022, Article No. 151312. doi: 10.1016/j.scitotenv.2021.151312

59. Singh, N.; Hui, D.; Singh, R.; Ahuja, I. P. S.; Feo, L.; and Fraternali, F., “Recycling of Plastic Solid Waste: A State of Art Review and Future Applications,” Composites Part B: Engineering, V. 115, Apr. 2017, pp. 409-422. doi: 10.1016/j.compositesb.2016.09.013

60. Gewert, B.; Plassmann, M. M.; and MacLeod, M., “Pathways for Degradation of Plastic Polymers Floating in the Marine Environment,” Environmental Science: Processes & Impacts, V. 17, No. 9, Sept. 2015, pp. 1513-1521. doi: 10.1039/C5EM00207A

61. Ebnesajjad, S., and Ebnesajjad, C. F., Surface Treatment of Materials for Adhesion Bonding, first edition, William Andrew Publishing, Norwich, NY, 2006, 276 pp.

62. Morris, J. C., “The Acid Ionization Constant of HOCl from 5 to 35°,” The Journal of Physical Chemistry, V. 70, No. 12, Dec. 1966, pp. 3798-3805. doi: 10.1021/j100884a007

63. Held, A. M.; Halko, D. J.; and Hurst, J. K., “Mechanisms of Chlorine Oxidation of Hydrogen Peroxide,” Journal of the American Chemical Society, V. 100, No. 18, Aug. 1978, pp. 5732-5740. doi: 10.1021/ja00486a025

64. Pişkin, B., and Türkün, M., “Stability of Various Sodium Hypochlorite Solutions,” Journal of Endodontics, V. 21, No. 5, May 1995, pp. 253-255. doi: 10.1016/S0099-2399(06)80991-X

65. Gambarini, G.; De Luca, M.; and Gerosa, R., “Chemical Stability of Heated Sodium Hypochlorite Endodontic Irrigants,” Journal of Endodontics, V. 24, No. 6, June 1998, pp. 432-434. doi: 10.1016/S0099-2399(98)80027-7

66. Marion, J. J. C.; Manhães, F. C.; Bajo, H.; and Duque, T. M., “Efficiency of Different Concentrations of Sodium Hypochlorite During Endodontic Treatment. Literature Review,” Dental Press Endodontics, V. 2, No. 4, Oct.-Dec. 2012, pp. 32-37.

67. Wright, P. P.; Kahler, B.; and Walsh, L. J., “Alkaline Sodium Hypochlorite Irrigant and Its Chemical Interactions,” Materials, V. 10, No. 10, Oct. 2017, Article No. 1147.

68. Umeda, K.; Miyasako, T.; Sugiyama, A.; Tanaka, A.; Suzuki, M.; Tokumitsu, E.; and Shimoda, T., “Impact of UV/O3 Treatment on Solution- Processed Amorphous InGaZnO4 Thin-Film Transistors,” Journal of Applied Physics, V. 113, No. 18, May 2013, Article No. 184509. doi: 10.1063/1.4804667

69. Le-The, H.; Tiggelaar, R. M.; Berenschot, E.; van den Berg, A.; Tas, N.; and Eijkel, J. C. T., “Postdeposition UV-Ozone Treatment: An Enabling Technique to Enhance the Direct Adhesion of Gold Thin Films to Oxidized Silicon,” ACS Nano, V. 13, No. 6, June 2019, pp. 6782-6789. doi: 10.1021/acsnano.9b01403

70. Cauich-Cupul, J. I.; Herrera-Franco, P. J.; García-Hernández, E.; Moreno-Chulim, V.; and Valadez-González, A., “Factorial Design Approach to Assess the Effect of Fiber–Matrix Adhesion on the IFSS and Work of Adhesion of Carbon Fiber/Polysulfone-Modified Epoxy Composites,” Carbon Letters, V. 29, No. 4, Aug. 2019, pp. 345-358. doi: 10.1007/s42823-019-00039-7

71. Pritchard, G., “Coupling Agents,” Plastics Additives: An A-Z Reference, G. Pritchard, ed., Springer, Dordrecht, the Netherlands, 1998, pp. 189-196.

72. Helmy, R., “Reaction of Organosilicon Hydrides with Inorganic Surfaces: An Example of Surface Catalyzed Self-Assembly and Water Porosimetry: A New Technique to Characterize Hydrophobic Porous Surfaces and Wetting in Nano-Confinement,” PhD dissertation, Seton Hall University, South Orange, NJ, 2005, 161 pp.

73. Tyagi, G.; Singhal, A.; Routroy, S.; Bhunia, D.; and Lahoti, M., “Radiation Shielding Concrete with Alternate Constituents: An Approach to Address Multiple Hazards,” Journal of Hazardous Materials, V. 404, Part B, Feb. 2021, Article No. 124201. doi: 10.1016/j.jhazmat.2020.124201

74. Choi, Y. W.; Moon, D. J.; Kim, Y. J.; and Lachemi, M., “Characteristics of Mortar and Concrete Containing Fine Aggregate Manufactured from Recycled Waste Polyethylene Terephthalate Bottles,” Construction and Building Materials, V. 23, No. 8, Aug. 2009, pp. 2829-2835. doi: 10.1016/j.conbuildmat.2009.02.036


ALSO AVAILABLE IN:

Electronic Materials Journal