Retrofitting Exterior Reinforced Concrete Beam-Column Joints with Transverse Beams Using Fiber-Reinforced Polymer

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Retrofitting Exterior Reinforced Concrete Beam-Column Joints with Transverse Beams Using Fiber-Reinforced Polymer

Author(s): Altho Sagara, Iswandi Imran, Erwin Lim, and Patria Kusumaningrum

Publication: Structural Journal

Volume: 123

Issue: 1

Appears on pages(s): 119-130

Keywords: exterior beam-column joint; fiber-reinforced polymer (FRP); joint hoops; joint shear strength; retrofitting

DOI: 10.14359/51749100

Date: 1/1/2026

Abstract:
During past earthquakes, failures of beam-column joints have commonly been observed on the exteriors of buildings. However, only one side of these joints can be retrofitted because of the presence of beams on the other three sides. Therefore, this study aims to test four exterior beam-column joints with transverse beams, leaving the rear side as the only viable location for placing fiber-reinforced polymer (FRP) laminate. All four test specimens were designed with insufficient joint shear strength, as determined by ACI 318-19 equations, while satisfying the criteria for a strong-column/weak-beam mechanism and sufficient development length for bar anchorage. A total of two un-retrofitted specimens, with and without joint hoops, were constructed as controls. Subsequently, two similar specimens were retrofitted by applying FRP laminate on the rear side. The results show that sufficient FRP laminate can enhance the seismic performance of joints in terms of deformability, energy dissipation, and failure delay.

Related References:

1. Nugroho, W. O.; Sagara, A.; and Imran, I., “The Evolution of Indonesian Seismic and Concrete Building Codes: From the Past to the Present,” Structures, V. 41, July 2022, pp. 1092-1108.

2. Zaidir, F.; Hakam, A.; and Ismail, F. A., “Repair and Strengthening of Building after 2009 West Sumatera Earthquake,” Proceedings of PIT KE-5 IABI Disaster Research National Seminar, Andalas University, Padang, West Sumatra, 2018, pp. 731-742. (in Indonesian)

3. Hanson, N. W., and Connor, H. W., “Seismic Resistance of Reinforced Concrete Beam-Column Joints,” Journal of the Structural Division, ASCE, V. 93, No. 5, Oct. 1967, pp. 533-560. doi: 10.1061/JSDEAG.0001785

4. Bayhan, B.; Moehle, J. P.; Yavari, S.; Elwood, K. J.; Lin, S. H.; Wu, C. L.; and Hwang, S. J., “Seismic Response of a Concrete Frame with Weak Beam-Column Joints,” Earthquake Spectra, V. 31, No. 1, Feb. 2015, pp. 293-315. doi: 10.1193/071811EQS179M

5. Hassan, W. M., and Moehle, J. P., “Shear Strength of Exterior and Corner Beam-Column Joints without Transverse Reinforcement,” ACI Structural Journal, V. 115, No. 6, Nov. 2018, pp. 1719-1728. doi: 10.14359/51702416

6. Pantelides, C. P.; Hansen, J.; Ameli, M. J.; and Reaveley, L. D., “Seismic Performance of Reinforced Concrete Building Exterior Joints with Substandard Details,” Journal of Structural Integrity and Maintenance, V. 2, No. 1, 2017, pp. 1-11. doi: 10.1080/24705314.2017.1280589

7. Hwang, S.-J.; Lee, H.-J.; Liao, T.-F.; Wang, K.-C.; and Tsai, H.-H., “Role of Hoops on Shear Strength of Reinforced Concrete Beam-Column Joints,” ACI Structural Journal, V. 102, No. 3, May-June 2005, pp. 445-453.

8. Al-Osta, M. A.; Khan, U.; Baluch, M. H.; and Rahman, M. K., “Effects of Variation of Axial Load on Seismic Performance of Shear Deficient RC Exterior BCJs,” International Journal of Concrete Structures and Materials, V. 12, No. 1, 2018, Article No. 46. doi: 10.1186/s40069-018-0277-0

9. Castro, J. J., and Imai, H., “Structural Performance of Exterior Beam Column Joints with Mechanical Anchorage at Main Bars,” Proceedings of the 13th World Conference on Earthquake Engineering (13WCEE), Vancouver, BC, Canada, Aug. 2004, Paper No. 2474.

10. Kuang, J. S., and Wong, H. F., “Effectiveness of Horizontal Stirrups in Joint Core for Exterior Beam-Column Joints with Nonseismic Design,” Procedia Engineering, V. 14, 2011, pp. 3301-3307.

11. Alsayed, S. H.; Al-Salloum, Y. A.; Almusallam, T. H.; and Siddiqui, N. A., “Seismic Response of FRP-Upgraded Exterior RC Beam-Column Joints,” Journal of Composites for Construction, ASCE, V. 14, No. 2, Apr. 2010, pp. 195-208. doi: 10.1061/(ASCE)CC.1943-5614.0000067

12. Alaee, P., and Li, B., “High-Strength Concrete Exterior Beam-Column Joints with High-Yield Strength Steel Reinforcements,” Engineering Structures, V. 145, Aug. 2017, pp. 305-321. doi: 10.1016/j.engstruct.2017.05.024

13. Bindhu, K. R.; Sukumar, P. M.; and Jaya, K. P., “Performance of Exterior Beam-Column Joints Under Seismic Type Loading,” ISET Journal of Earthquake Technology, V. 46, No. 2, June 2009, Paper No. 503, pp. 47-64

14. Lee, H.-J., and Chang, C.-J., “High-Strength Reinforcement in Exterior Beam-Column Joints under Cyclic Loading,” ACI Structural Journal, V. 114, No. 5, Sept.-Oct. 2017, pp. 1325-1338. doi: 10.14359/51700788

15. Ehsani, M. R., and Wight, J. K., “Exterior Reinforced Concrete Beam-to-Column Connections Subjected to Earthquake-Type Loading,” ACI Journal Proceedings, V. 82, No. 4, July-Aug. 1985, pp. 492-499.

16. Canbolat, B. B., and Wight, J. K., “Experimental Investigation on Seismic Behavior of Eccentric Reinforced Concrete Beam-Column-Slab Connections,” ACI Structural Journal, V. 105, No. 2, Mar.-Apr. 2008, pp. 154-162.

17. Lee, H.-J., and Yu, S.-Y., “Cyclic Response of Exterior Beam-Column Joints with Different Anchorage Methods,” ACI Structural Journal, V. 106, No. 3, May-June 2009, pp. 329-339.

18. Hakuto, S.; Park, R.; and Tanaka, H., “Seismic Load Tests on Interior and Exterior Beam-Column Joints with Substandard Reinforcing Details,” ACI Structural Journal, V. 97, No. 1, Jan.-Feb. 2000, pp. 11-25.

19. Li, B.; Lam, E. S.-S.; Wu, B.; and Wang, Y.-Y., “Effect of High Axial Load on Seismic Behavior of Reinforced Concrete Beam-Column Joints with and without Strengthening,” ACI Structural Journal, V. 112, No. 6, Nov.-Dec. 2015, pp. 713-723. doi: 10.14359/51687938

20. Engindeniz, M.; Kahn, L F..; and Zureick, A.-H., “Repair and Strengthening of Reinforced Concrete Beam-Column Joints: State of the Art,” ACI Structural Journal, V. 102, No. 2, Mar.-Apr. 2005, pp. 1-14.

21. El-Amoury, T., and Ghobarah, A., “Seismic Rehabilitation of Beam–Column Joint Using GFRP Sheets,” Engineering Structures, V. 24, No. 11, Nov. 2002, pp. 1397-1407.

22. Attari, N.; Si Youcef, Y.; and Amziane, S., “Seismic Performance of Reinforced Concrete Beam–Column Joint Strengthening by FRP Sheets,” Structures, V. 20, Aug. 2019, pp. 353-364. doi: 10.1016/j.istruc.2019.04.007

23. Maheri, M. R., and Torabi, A., “Retrofitting External RC Beam-Column Joints of an Ordinary MRF Through Plastic Hinge Relocation Using FRP Laminates,” Structures, V. 22, Dec. 2019, pp. 65-75. doi: 10.1016/j.istruc.2019.08.004

24. Mahmoud, M. H.; Afefy, H. M.; Kassem, N. M.; and Fawzy, T. M., “Strengthening of Defected Beam–Column Joints Using CFRP,” Journal of Advanced Research, V. 5, No. 1, Jan. 2014, pp. 67-77. doi: 10.1016/j.jare.2012.11.007

25. ACI Committee 440, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-17),” American Concrete Institute, Farmington Hills, MI, 2017, 112 pp.

26. ACI Committee 374, “Acceptance Criteria for Moment Frames Based on Structural Testing and Commentary (ACI 374.1-05) (Reapproved 2019),” American Concrete Institute, Farmington Hills, MI, 2005, 9 pp.

27. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

28. Hwang, S.-J., and Lee, H.-J., “Analytical Model for Predicting Shear Strengths of Exterior Reinforced Concrete Beam-Column Joints for Seismic Resistance,” ACI Structural Journal, V. 96, No. 5, Sept.-Oct. 1999, pp. 846-858.

29. Richart, F. E.; Brandtzaeg, A.; and Brown, R. L., “A Study of the Failure of Concrete Under Combined Compressive Stresses,” University of Illinois Engineering Experiment Station, Urbana, IL, Nov. 1928, 110 pp.

30. del Rey Castillo, E.; Kanitkar, R.; Smith, S. T.; Griffith, M. C.; and Ingham, J. M., “Design Approach for FRP Spike Anchors in FRP-Strengthened RC Structures,” Composite Structures, V. 214, Apr. 2019, pp. 23-33. doi: 10.1016/j.compstruct.2019.01.100


ALSO AVAILABLE IN:

Electronic Structural Journal