Title: Slab-on-Ground Analysis for Storage Rack Concentrated Uplift Loading (Prepublished)

Author(s): Nathan Bissonnette

Publication: Structural Journal

Volume:

Issue:

Appears on pages(s):

Keywords: model concrete; seismic uplift; slab-on-ground; storage racks

DOI: 10.14359/51746820

Date: 5/15/2025

Abstract:
Slabs-on-ground supporting storage racks are often subjected to concentrated uplift under building code seismic forces. While methods for determining slab-on-ground capacity for downward loads are well defined, guidance for resistance to uplift has been limited and relies on finite element analysis. A simplified approach is presented for calculating slab-on-ground uplift capacity as a function of slab thickness, reinforcing content, and storage rack frame depth. Testing is conducted on small-scale concrete samples in bending to obtain the material properties. Model slabs are created and tested for an upward and downward force couple representing concentrated seismic uplift on a reinforced slab-on-ground. The plastic hinge failure mechanism of the slab samples is correlated with finite element models, and straightforward formulas are developed to produce a table of uplift capacities for common storage rack and slab-on-ground configurations.


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer