Nonlinear Finite Element Analysis of Interface Shear Transfer in Various Testing Methods

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Nonlinear Finite Element Analysis of Interface Shear Transfer in Various Testing Methods

Author(s): Adham Abu-Abaileh and Matthew Soltani

Publication: Structural Journal

Volume: 123

Issue: 1

Appears on pages(s): 61-74

Keywords: clamping force concept; cohesive forces evaluation; connection geometry variability; empirical validation methods; interface crack propagation; material property definition enhancements; shear-friction mechanisms

DOI: 10.14359/51746757

Date: 1/1/2026

Abstract:
This study employs advanced nonlinear finite element (FE) modeling to investigate interface shear transfer (IST) behavior in reinforced concrete connections, a crucial factor for bridge durability and safety. The research examines shear-transfer mechanisms at the interface between precast girders and cast-in-place deck segments through three experimental methods: beam, pushoff, and Iosipescu four-point bending tests. FE simulations evaluated stress distributions, IST capacity, and failure mechanisms. Validation against experimental data shows that the Iosipescu test provides the most accurate representation of IST behavior, exhibiting a stress distribution error margin of only 1%, closely aligned with observed failure patterns. In contrast, the pushoff test showed a 30% deviation from empirical data, indicating reduced accuracy in predicting real-world IST behavior. These findings highlight the importance of incorporating the Iosipescu test into IST evaluation protocols, as its greater precision enhances design methodologies for concrete bridges, reduces structural failure risks, and informs future updates to IST-related codes.

Related References:

1. Soltani, M., “Interface Shear Transfer in Reinforced Concrete Members: Code Evaluation, Modeling, and Testing,” doctoral dissertation, Clemson University, Clemson, SC, 2016.

2. Soltani, M., and Ross, B. E., “Evaluation of a Four-Point Bending-Test Method for Interface Shear Transfer in Concrete Members,” Practice Periodical on Structural Design and Construction, ASCE, V. 22, No. 4, 2017, p. 04017008.

3. Ayub, M., “Investigation of March 15, 2018 Pedestrian Bridge Collapse at Florida International University, Miami, FL - July 2019,” Occupational Safety and Health Administration, Washington, DC, 2018, 115 pp.

4. Jimenez-Perez, R.; Gergely, P.; and White, R. N., “Shear Transfer Across Cracks in Reinforced Concrete,” Cornell University, Ithaca, NY, 1978.

5. Santos, P. M. D., and Júlio, E. N. B. S., “A State-of-the-Art Review on Shear-Friction,” Engineering Structures, V. 45, 2012, pp. 435-448.

6. AASHTO, “AASHTO LRFD Bridge Design Specifications,” ninth edition, American Association of State Highway and Transportation Officials, Washington, DC, 2020.

7. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

8. Soltani, M., “Reliability Analyses of Interface Shear Transfer in AASHTO LRFD Specifications Model and an Alternative Model,” PCI Journal, V. 63, No. 5, 2018, pp. 36-50.

9. Mast, R. F., “Auxiliary Reinforcement in Concrete Connections,” Journal of the Structural Division, ASCE, V. 94, No. 6, 1968, pp. 1485-1504.

10. Birkeland, P. W., and Birkeland, H. W., “Connections in Precast Concrete Construction,” ACI Journal Proceedings, V. 63, No. 3, Mar. 1966, pp. 345-368.

11. Mattock, A. H., and Hawkins, N. M., “Shear Transfer in Reinforced Concrete - Recent Research,” PCI Journal, V. 17, No. 2, 1972, pp. 55-75.

12. Kahn, L. F., and Mitchell, A. D., “Shear Friction Tests with High-Strength Concrete,” ACI Structural Journal, V. 99, No. 1, Jan.-Feb. 2002, pp. 98-103.

13. Hsu, T. T. C.; Mau, S. T.; and Chen, B., “Theory on Shear Transfer Strength of Reinforced Concrete,” ACI Structural Journal, V. 84, No. 2, Mar.-Apr. 1987, pp. 149-160.

14. Santos, P., and Júlio, E. N., “Interface Shear Transfer on Composite Concrete Members,” ACI Structural Journal, V. 111, No. 1, Jan.-Feb. 2014, pp. 113-122.

15. Tsoukantas, S. G., and Tassios, T. P., “Shear Resistance of Connections Between Reinforced Concrete Linear Precast Elements,” ACI Structural Journal, V. 86, No. 3, May-June 1989, pp. 242-249.

16. BS EN 1992-1-1, “Eurocode 2: Design of Concrete Structures: Part 1-1: General Rules and Rules for Buildings,” British Standards Institution, London, UK, 2004.

17. CSA A23.3:24, “Design of Concrete Structures,” CSA Group, Toronto, ON, Canada, 2012.

18. Hofbeck, J. A.; Ibrahim, I. O.; and Mattock, A. H., “Shear Transfer in Reinforced Concrete,” ACI Journal Proceedings, V. 66, No. 2, Feb. 1969, pp. 119-128.

19. Mattock, A. H.; Li, W. K.; and Wang, T. C., “Shear Transfer in Lightweight Reinforced Concrete,” PCI Journal, V. 21, No. 1, 1976, pp. 20-39.

20. Walraven, J.; Frenay, J.; and Pruijssers, A., “Influence of Concrete Strength and Load History on the Shear Friction Capacity of Concrete Members,” PCI Journal, V. 32, No. 1, 1987, pp. 66-84.

21. Iosipescu, N., “New Accurate Procedure for Single Shear Testing of Metals,” Journal of Materials, V. 2, No. 3, 1967, pp. 537-56.

22. Loov, R. E., and Patnaik, A. K., “Horizontal Shear Strength of Composite Concrete Beams with a Rough Interface,” PCI Journal, V. 39, No. 1, 1994, pp. 48-69.

23. Tao, Y., and Chen, J.-F., “Concrete Damage Plasticity Model for Modeling FRP-to-Concrete Bond Behavior,” Journal of Composites for Construction, ASCE, V. 19, 2015, p. 04014026.

24. Yang, Z. J., and Proverbs, D., “A Comparative Study of Numerical Solutions to Non-Linear Discrete Crack Modelling of Concrete Beams Involving Sharp Snap-Back,” Engineering Fracture Mechanics, V. 71, No. 1, 2004, pp. 81-105.

25. Rots, J. G., “Smeared and Discrete Representations of Localized Fracture,” International Journal of Fracture, V. 51, Sept. 1991, pp. 45-59.

26. Yang, Z. J.; Chen, J. F.; and Proverbs, D., “Finite Element Modelling of Concrete Cover Separation Failure in FRP Plated RC Beams,” Construction and Building Materials, V. 17, No. 1, 2003, pp. 3-13.

27. Yang, Z. J., and Chen, J., “Finite Element Modelling of Multiple Cohesive Discrete Crack Propagation in Reinforced Concrete Beams,” Engineering Fracture Mechanics, V. 72, No. 14, 2005, pp. 2280-2297.

28. Yang, Z. J.; Su, X. T.; and Chen, J. F., “Monte Carlo Simulation of Complex Cohesive Fracture in Random Heterogeneous Quasi-Brittle Materials,” International Journal of Solids and Structures, V. 46, No. 17, 2009, pp. 3222-3234.

29. Planas, P., and Bazant, Z. P., Fracture and Size Effect in Concrete and Other Quasibrittle Materials, Routledge, NY, Mar. 2019, 640 pp.

30. Rots, J. “Computational Modeling of Concrete Fracture,” doctoral thesis, Delft University of Technology, Delft, the Netherlands, 1988.

31. Bažant, Z. P., and Oh, B. H., “Crack Band Theory for Fracture of Concrete,” Materiales de Construcción, V. 16, No. 3, 1983, pp. 155-177.

32. Hordijk, D. A., “Local Approach to Fatigue of Concrete,” doctoral thesis, Delft University of Technology, Delft, the Netherlands, Oct. 1991.

33. fib, “fib Model Code for Concrete Structures 2010,” International Federation for Structural Concrete, Lausanne, Switzerland, 2013, 434 pp. 10.1002/9783433604090.

34. Dassault Systèmes, “Abaqus Unified FEA,” Vélizy-Villacoublay, France, https://www.3ds.com/products-services/simulia/products/abaqus. (last accessed Nov. 7, 2025)

35. Lee, J., and Fenves, G. L., “Plastic-Damage Model for Cyclic Loading of Concrete Structures,” Journal of Engineering Mechanics, ASCE, V. 124, No. 8, 1998, pp. 892-900.

36. Sanez, L. P., “Discussion of Equation for the Stress-Strain Curve of Concrete By Desayi and Krishnan,” ACI Journal Proceedings, V. 61, No. 9, Sept. 1964, pp. 1229-1235.

37. Malm, R., “Shear Cracks in Concrete Structures Subjected to In-Plane Stresses,” thesis, Royal Institute of Technology, Stockholm, Sweden, 2006.

38. Soltani, M., and Ross, B. E., “Database Evaluation of Interface Shear Transfer in Reinforced Concrete Members,” ACI Structural Journal, V. 114, No. 2, Mar.-Apr. 2017, pp. 383-394

39. Patnaik, A., “Behavior of Composite Concrete Beams with Smooth Interface,” Journal of Structural Engineering, ASCE, V. 127, No. 4, 2001, pp. 359-366.

40. Shaw, D. M., and Sneed, L. H., “Interface Shear Transfer of Lightweight-Aggregate Concretes Cast at Different Times,” PCI Journal, V. 59, No. 3, 2014, pp. 130-144.

41. Dassault Systèmes, “Abaqus Analysis User’s Manual,” Version 6.13, Vélizy-Villacoublay, France, 2013.


ALSO AVAILABLE IN:

Electronic Structural Journal